In situ observation of heterogeneous melting of poly[(R)-3-hydroxybutyrate] single crystals by temperature-controlled atomic force microscopy

被引:17
作者
Fujita, M
Iwata, T
Doi, Y
机构
[1] Riken Inst Phys & Chem Res, Polymer Chem Lab, Wako, Saitama 3510198, Japan
[2] Tokyo Inst Technol, Dept Innovat & Engineered Mat, Midori Ku, Yokohama, Kanagawa 2268501, Japan
关键词
poly[(R)-3-hydroxybutyrate; single crystal; annealing; melting; in situ AFM;
D O I
10.1016/S0141-3910(03)00082-X
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Morphological changes of lath-shaped single crystals of poly[(R)-3-hydroxybutyrate] (P(3HB)) during annealing were followed in situ by a temperature-controlled atomic force microscopy (TC-AFM) in order to elucidate thermal stability or chain-mobility within the individual single crystal. Two kinds of the solution-grown single crystals prepared under different crystallization conditions were used to also investigate the influence of crystallization temperature on the annealing behavior. The significant morphological changes during annealing were observed at temperatures above the original crystallization temperature. The TC-AFM observations have revealed that ridges on the lamellar surface running across the crystal width (parallel to the b-axis), and cracks along the long axis of the crystal (parallel to the a-axis) are occasionally formed by thermal treatment. At a higher annealing temperature, numerous notches along the b-axis were frequently formed at the lateral sides of crystal. The notch formation may be due to preferential melting of the defective or less perfect regions within the lamellar crystal. The whole crystal became narrow while the notches progressed along b-axis, and some cavities developed at the central portion of the crystal as annealing temperature was elevated. The isothermal annealing experiment has demonstrated that the melting of P(3HB) crystals gradually progresses from the lateral outer faces. On the basis of the results, it has been concluded that the less perfect regions along the a-axis and b-axis exist within the P(3HB) single crystal, and that melting of the regions at the lateral sides of crystal is more easily initiated. (C). 2003 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:131 / 139
页数:9
相关论文
共 39 条
  • [1] Solid-state structures and enzymatic degradabilities for melt-crystallized films of copolymers of (R)-3-hydroxybutyric acid with different hydroxyalkanoic acids
    Abe, H
    Doi, Y
    Aoki, H
    Akehata, T
    [J]. MACROMOLECULES, 1998, 31 (06) : 1791 - 1797
  • [2] Crystal melting and its kinetics on poly(ethylene oxide) by in situ atomic force microscopy
    Beekmans, LGM
    van der Meer, DW
    Vancso, GJ
    [J]. POLYMER, 2002, 43 (06) : 1887 - 1895
  • [3] MORPHOLOGY OF SINGLE-CRYSTALS OF POLY(HYDROXYBUTYRATE) AND COPOLYMERS OF HYDROXYBUTYRATE AND HYDROXYVALERATE
    BIRLEY, C
    BRIDDON, J
    SYKES, KE
    BARKER, PA
    ORGAN, SJ
    BARHAM, PJ
    [J]. JOURNAL OF MATERIALS SCIENCE, 1995, 30 (03) : 633 - 638
  • [4] DOI Y, 1990, MACROMOLECULES, V23, P26, DOI 10.1021/ma00203a006
  • [5] DOI Y, 1995, MACROMOLECULES, V28, P4822, DOI 10.1021/ma00118a007
  • [6] Doi Y., 1990, MICROBIAL POLYESTERS
  • [7] Structure and morphology of the aliphatic polyester poly-β-propiolactone in solution-grown chain-folded lamellar crystals
    Furuhashi, Y
    Iwata, T
    Sikorski, P
    Atkins, E
    Doi, Y
    [J]. MACROMOLECULES, 2000, 33 (25) : 9423 - 9431
  • [8] GEIL PH, 1963, POLYM SINGLE CRYSTAL
  • [9] Enzymatic degradation of single crystals of bacterial and synthetic poly(beta-hydroxybutyrate)
    Hocking, PJ
    Marchessault, RH
    Timmins, MR
    Lenz, RW
    Fuller, RC
    [J]. MACROMOLECULES, 1996, 29 (07) : 2472 - 2478
  • [10] Iwata T, 1999, MACROMOL CHEM PHYSIC, V200, P2429, DOI 10.1002/(SICI)1521-3935(19991101)200:11<2429::AID-MACP2429>3.0.CO