Hardness and plastic deformation in a bulk metallic glass

被引:266
作者
Ramamurty, U [1 ]
Jana, S
Kawamura, Y
Chattopadhyay, K
机构
[1] Indian Inst Sci, Dept Met, Bangalore 560012, Karnataka, India
[2] Kumamoto Univ, Dept Mech Engn & Mat Sci, Kumamoto 8608555, Japan
关键词
bulk amorphous materials; hardness; plastic deformation; shear bands; crystallization;
D O I
10.1016/j.actamat.2004.10.023
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
An experimental investigation into the Vickers hardness and associated plastic deformation in as-east and annealed Pd42Ni40P18 bulk metallic glass was conducted. In addition to the bulk indentation behavior. the deformation morphology underneath the indenter and its variation with annealing time was examined by employing the bonded interface technique. For both the bulk and the interface indentations, the trends in the shear band induced plastic deformation zone sizes with the indentation load agree well with those predicted from the expanding cavity model. However, the yield strength extracted from the indentation data is higher than that measured in uniaxial compression, indicating pressure sensitive plasticity. Results show that the as-east as well as the partiailly crystallized alloys deform appreciably through the shear band mechanism, with semi-circular and radial shear band morphologies. The latter gets increasingly prominent with increasing annealing time. Atomic force microscopy of the deformation region reveals increasing shear band heights with load, consistent with nanoindentation results. whereas the spacing between semicircular shear bands was found to be independent of their distance from the tip of the indenter for the as-east alloy. it was found to increase linearly, after a small zone of constant spacing, in the annealed alloys. Implications of this study in understanding the mechanical behavior of metallic glasses and their derivatives are discussed. (C) 2004 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:705 / 717
页数:13
相关论文
共 40 条
[1]   Microstructure and mechanical properties of a partially crystallized La-based bulk metallic glass [J].
Basu, J ;
Nagendra, N ;
Li, Y ;
Ramamurty, U .
PHILOSOPHICAL MAGAZINE, 2003, 83 (15) :1747-1760
[2]   Shear bands and cracking of metallic glass plates in bending [J].
Conner, RD ;
Johnson, WL ;
Paton, NE ;
Nix, WD .
JOURNAL OF APPLIED PHYSICS, 2003, 94 (02) :904-911
[3]   Computational modeling of the forward and reverse problems in instrumented sharp indentation [J].
Dao, M ;
Chollacoop, N ;
Van Vliet, KJ ;
Venkatesh, TA ;
Suresh, S .
ACTA MATERIALIA, 2001, 49 (19) :3899-3918
[4]   HARDNESS/STRENGTH RATIO OF METALLIC GLASSES [J].
DAVIS, LA .
SCRIPTA METALLURGICA, 1975, 9 (04) :431-435
[5]   PLASTIC-FLOW AND FRACTURE OF PD40NI40P20 METALLIC-GLASS UNDER AN INDENTOR [J].
DONOVAN, PE .
JOURNAL OF MATERIALS SCIENCE, 1989, 24 (02) :523-535
[6]   A YIELD CRITERION FOR PD40NI40P20 METALLIC-GLASS [J].
DONOVAN, PE .
ACTA METALLURGICA, 1989, 37 (02) :445-456
[7]   TERNARY COMPOUND IN THE PD-NI-P ALLOY SYSTEM [J].
DONOVAN, PE ;
EVANS, PV ;
GREER, AL .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1986, 5 (09) :951-952
[8]   CONE INDENTATION EXPERIMENTS [J].
DUGDALE, DS .
JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 1954, 2 (04) :265-277
[9]  
DUGDALE DS, 1955, J MECH PHYS SOLIDS, V3, P197, DOI 10.1016/0022-5096(55)90011-9
[10]   Nanocrystalline composites with high strength obtained in Zr-Ti-Ni-Cu-Al bulk amorphous alloys [J].
Fan, C ;
Louzguine, DV ;
Li, CF ;
Inoue, A .
APPLIED PHYSICS LETTERS, 1999, 75 (03) :340-342