Adhesion behaviour assessment on diamond coated silicon nitride by acoustic emission

被引:48
作者
Belmonte, M [1 ]
Fernandes, AJS
Costa, FM
Oliveira, FJ
Silva, RF
机构
[1] Univ Aveiro, CICECO, Dept Ceram & Glass Engn, P-3810193 Aveiro, Portugal
[2] Univ Aveiro, Dept Phys, P-3810193 Aveiro, Portugal
关键词
diamond film; adhesion; mechanical properties characterization; acoustic properties;
D O I
10.1016/S0925-9635(02)00305-9
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Acoustic emission (AE) from cracking events in microwave plasma assisted chemical vapour deposition diamond coated Si3N4 ceramics during Brale indentation tests was investigated. The experiments were conducted in a modified macro-indentation technique, that avoids the discrete loading limitation of conventional indentation by using a constant indenter displacement rate. The recorded AE signals, in conjunction with scanning electron microscope post-observations of the cracking pattern, allowed the adhesion behaviour investigation of the diamond film/ceramic system. The AE graphs evidenced that the most intensive acoustic peaks arise when film spalling takes place. The Si3N4 surface roughness was used as a variable to confirm the feasibility of the method. A better adhesion performance was achieved for the substrate with a higher roughness. For the diamond coated as ground substrate the critical load for film detachment is similar to 1000 N, while the film adhesion on the coated polished material is weaker. The assessment of the interfacial cracking resistance of the films gives a maximum value of 1372 kN m(-1). (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:733 / 737
页数:5
相关论文
共 15 条
[1]  
BELMONTE M, UNPUB
[2]   Interlayers for diamond deposition on tool materials [J].
Endler, I ;
Leonhardt, A ;
Scheibe, HJ ;
Born, R .
DIAMOND AND RELATED MATERIALS, 1996, 5 (3-5) :299-303
[3]   QUASI-STATIC SOLID PARTICLE DAMAGE IN BRITTLE SOLIDS .1. OBSERVATIONS, ANALYSIS AND IMPLICATIONS [J].
EVANS, AG ;
WILSHAW, TR .
ACTA METALLURGICA, 1976, 24 (10) :939-956
[4]   THE ROLE OF CEMENTED WC SUBSTRATE MORPHOLOGY ON THE DIAMOND FILM GROWTH AND CRACKING RESISTANCE [J].
HUANG, TH ;
KUO, CT ;
LIN, TS .
SCRIPTA METALLURGICA ET MATERIALIA, 1992, 26 (09) :1481-1486
[5]  
Janhanmir S., 1994, FRICTION WEAR CERAMI
[6]   ADHESION AND TRIBOLOGICAL PROPERTIES OF DIAMOND FILMS ON VARIOUS SUBSTRATES [J].
KUO, CT ;
YEN, TY ;
HUANG, TH ;
HSU, SE .
JOURNAL OF MATERIALS RESEARCH, 1990, 5 (11) :2515-2523
[7]  
Lee SK, 1997, J AM CERAM SOC, V80, P2367, DOI 10.1111/j.1151-2916.1997.tb03129.x
[8]  
Mallika K, 2001, THIN SOLID FILMS, V396, P145, DOI 10.1016/S0040-6090(01)01262-7
[9]   Applications of ceramic cutting tools [J].
Mehrotra, PK .
ADVANCED CERAMIC TOOLS FOR MACHINING APPLICATION - III, 1998, 138-1 :1-24
[10]   Adhesion of diamond coatings on cemented carbides [J].
Nesladek, M ;
Vandierendonck, K ;
Quaeyhaegens, C ;
Kerkhofs, M ;
Stals, LM .
THIN SOLID FILMS, 1995, 270 (1-2) :184-188