Al2O3-ZrO2 composite coatings for thermal-barrier applications

被引:47
作者
Ramaswamy, P
Seetharamu, S
Varma, KBR
Rao, KJ
机构
[1] INDIAN INST SCI,MAT RES CTR,BANGALORE 560012,KARNATAKA,INDIA
[2] CENT POWER RES INST,MAT TECHNOL DIV,BANGALORE 560094,KARNATAKA,INDIA
关键词
composite; multilayer; Al2O3-ZrO2; TBCs;
D O I
10.1016/S0266-3538(96)00111-X
中图分类号
TB33 [复合材料];
学科分类号
摘要
Graded alternate layers of Al2O3 and 8% Y2O3-ZrO2 and their admixtures were plasma sprayed onto bond-coated mild steel. They were evaluated for thermal-shock resistance, thermal-barrier characteristics, hot corrosion resistance (molten NaCl corrodant) and depth of attack, adhesion strength and the presence of phases. Although front-back temperature drops of 423-623 K were observed, some of the coatings showed good adherence even after 100 thermal shack cycles. In the sequence of the graded layers, the oxide which is directly in contact with the bond coat appears to influence the properties especially in coatings of 150 and 300 mu m thickness. Molten NaCl readily attacks the films at high hot-face temperatures (1273 K for 1 h) and the adhesive strength falls significantly by 50-60%. Diffusion of alkaline elements is also found to depend on the chemical composition of the outer coating directly facing the molten corrodant. (C) 1997 Elsevier Science Limited.
引用
收藏
页码:81 / 89
页数:9
相关论文
共 16 条
[1]  
BENNETT A, 1986, MATER SCI TECH SER, V2, P257, DOI 10.1179/026708386790123378
[2]   THERMAL-PROPERTIES OF CERIA AND YTTRIA PARTIALLY STABILIZED ZIRCONIA THERMAL BARRIER COATINGS [J].
BRANDON, JR ;
TAYLOR, R .
SURFACE & COATINGS TECHNOLOGY, 1989, 39 (1-3) :143-151
[3]  
Bratton R. J., 1981, ADV CERAM, V3, P226
[4]   FABRICATION OF TRANSPARENT GAMMA-AL2O3 FROM NANOSIZE PARTICLES [J].
GALLAS, MR ;
HOCKEY, B ;
PECHENIK, A ;
PIERMARINI, GJ .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1994, 77 (08) :2107-2112
[5]   ON THE THERMAL CYCLING LIFE OF PLASMA-SPRAYED YTTRIA-STABILIZED ZIRCONIA COATINGS [J].
JOSHI, SV ;
SRIVASTAVA, MP .
SURFACE & COATINGS TECHNOLOGY, 1993, 56 (03) :215-224
[6]  
Lannutti J. J., 1985, Ceramics International, V11, P91, DOI 10.1016/0272-8842(85)90003-3
[7]  
LUGSCHEIDER E, 1987, ADV COATINGS TECHNOL, P105
[8]  
MCPHERSON R, 1981, INT C MET COAT SAN F
[9]   FAILURE MECHANISMS OF THERMAL BARRIER COATINGS EXPOSED TO ELEVATED-TEMPERATURES [J].
MILLER, RA ;
LOWELL, CE .
THIN SOLID FILMS, 1982, 95 (03) :265-273
[10]  
MILLER RA, 87288 NASA, P1