Indentation damage and mechanical properties of human enamel and dentin

被引:417
作者
Xu, HHK
Smith, DT
Jahanmir, S
Romberg, E
Kelly, JR
Thompson, VP
Rekow, ED
机构
[1] Natl Inst Stand & Technol, Amer Dent Assoc Hlth Fdn, Paffenbarger Res Ctr, Gaithersburg, MD 20899 USA
[2] Natl Inst Stand & Technol, Div Ceram, Gaithersburg, MD 20899 USA
[3] Univ Maryland, Sch Dent, Dept Oral Hlth Care Delivery, Stat Grp, Baltimore, MD 21201 USA
[4] USN, Sch Dent, Dept Prosthodont, Bethesda, MD 20889 USA
[5] Univ Maryland, Sch Dent, Dept Restorat Dent, Baltimore, MD 21201 USA
[6] Univ Med & Dent New Jersey, Dept Orthodont, Newark, NJ 07103 USA
关键词
crack; dentino-enamel junction; enamel rod; fracture toughness; tooth orientation; modulus;
D O I
10.1177/00220345980770030601
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Understanding the mechanical properties of human teeth is important to clinical tooth preparation and to the development of "tooth-like" restorative materials. Previous studies have focused on the macroscopic fracture behavior of enamel and dentin. In the present study, we performed indentation studies to understand the microfracture and deformation and the microcrack-microstructure interactions of teeth. It was hypothesized that crack propagation would be influenced by enamel rods and the dentino-enamel junction (DEJ), and the mechanical properties would be influenced by enamel rod orientation and tooth-to-tooth variation. Twenty-eight human third molars were used for the measurement of hardness, fracture toughness, elastic modulus, and energy absorbed during indentation. We examined the effect of enamel rod orientation by propagating cracks in the occlusal surface, and in the axial section in directions parallel and perpendicular to the occlusal surface. The results showed that the cracks in the enamel axial section were significantly longer in the direction perpendicular to the occlusal surface than parallel. The cracks propagating toward the DEJ were always arrested and unable to penetrate dentin. The fracture toughness of enamel was not single-valued but varied by a factor of three as a function of enamel rod orientation. The elastic modulus of enamel showed a significant difference between the occlusal surface and the axial section. It is concluded that the cracks strongly interact with the DEJ and the enamel rods, and that the mechanical properties of teeth are functions of microstructural orientations; hence, single values of properties (e.g., a single toughness value or a single modulus value) should not be used without information on microstructural orientation.
引用
收藏
页码:472 / 480
页数:9
相关论文
共 24 条
[1]  
*ASTM, 1991, ASTM STAND 3
[2]   TENSILE STRENGTH AND MODULUS OF ELASTICITY OF TOOTH STRUCTURE AND SEVERAL RESTORATIVE MATERIALS [J].
BOWEN, RL ;
RODRIGUEZ, MS .
JOURNAL OF THE AMERICAN DENTAL ASSOCIATION, 1962, 64 (03) :378-&
[3]   OBJECTIVE EVALUATION OF SHORT-CRACK TOUGHNESS CURVES USING INDENTATION FLAWS - CASE-STUDY ON ALUMINA-BASED CERAMICS [J].
BRAUN, LM ;
BENNISON, SJ ;
LAWN, BR .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1992, 75 (11) :3049-3057
[4]  
CRAIG R. G., 1958, JOUR DENTAL RES, V37, P661
[5]   COMPRESSIVE PROPERTIES OF ENAMEL, DENTAL CEMENTS, AND GOLD [J].
CRAIG, RG ;
JOHNSON, DW ;
PEYTON, FA .
JOURNAL OF DENTAL RESEARCH, 1961, 40 (05) :936-&
[6]   FRACTURE-TOUGHNESS OF HUMAN-DENTIN [J].
ELMOWAFY, OM ;
WATTS, DC .
JOURNAL OF DENTAL RESEARCH, 1986, 65 (05) :677-681
[7]   RELATIONSHIP BETWEEN HARDNESS DISCOLORATION AND MICROBIAL INVASION IN CARIOUS DENTIN [J].
FUSAYAMA, T ;
OKUSE, K ;
HOSODA, H .
JOURNAL OF DENTAL RESEARCH, 1966, 45 (04) :1033-+
[8]   FRACTURE-TOUGHNESS OF HUMAN-ENAMEL [J].
HASSAN, R ;
CAPUTO, AA ;
BUNSHAH, RF .
JOURNAL OF DENTAL RESEARCH, 1981, 60 (04) :820-827
[9]  
LAWN BR, 1993, FRACTURE BRITTLE SOL, pCH7
[10]   STRUCTURE-PROPERTY RELATIONS AND CRACK RESISTANCE AT THE BOVINE DENTIN-ENAMEL JUNCTION [J].
LIN, CP ;
DOUGLAS, WH .
JOURNAL OF DENTAL RESEARCH, 1994, 73 (05) :1072-1078