Evaluation of interface degradation during cyclic oxidation of EB-PVD thermal barrier coatings and correlation with TGO luminescence

被引:79
作者
Tolpygo, VK [1 ]
Clarke, DR
Murphy, KS
机构
[1] Univ Calif Santa Barbara, Dept Mat, Santa Barbara, CA 93106 USA
[2] Howmet Res Corp, Whitehall, MI 49461 USA
关键词
thermal barrier coatings; spallation failure; cyclic oxidation; bond coat;
D O I
10.1016/j.surfcoat.2004.08.001
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The typical degradation mechanism of EB-PVD thermal barrier coatings (TBCs) that occurs during cyclic furnace testing of a commercial 7YSZ coating on a single-crystal nickel-base superalloy is analyzed. The mechanism includes local separation of the ceramic top coat from the thermally grown oxide (TGO), growth of the separated regions along the coating-substrate interface, and, upon reaching a critical size, large-scale TBC spallation. The extent of interface separation was evaluated by analyzing cross-section microstructures of the tested samples at different stages of TBC cyclic life. The morphological changes of the TGO as a result of roughening of the (Ni,Pt)Al bond coat surface were also quantified. Concurrently, the evolution of the TGO luminescence during cyclic oxidation and the development of TBC undulations, associated with large TBC-TGO interface separations, were monitored. It is demonstrated that there is a correlation between the extent of interface damage and the shift in TGO luminescence frequency, which can be evaluated nondestructively. (C) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:62 / 70
页数:9
相关论文
共 19 条
[1]   Variability of stress in alumina corrosion layers formed in thermal-barrier coatings [J].
Atkinson, A ;
Selçuk, A ;
Webb, SJ .
OXIDATION OF METALS, 2000, 54 (5-6) :371-384
[2]   Nondestructive evaluation of the oxidation stresses through thermal barrier coatings using Cr3+ piezospectroscopy [J].
Christensen, RJ ;
Lipkin, DM ;
Clarke, DR ;
Murphy, K .
APPLIED PHYSICS LETTERS, 1996, 69 (24) :3754-3756
[3]   Mechanisms controlling the durability of thermal barrier coatings [J].
Evans, AG ;
Mumm, DR ;
Hutchinson, JW ;
Meier, GH ;
Pettit, FS .
PROGRESS IN MATERIALS SCIENCE, 2001, 46 (05) :505-553
[4]   On the measurement of strain in coatings formed on a wrinkled elastic substrate [J].
Gong, XY ;
Clarke, DR .
OXIDATION OF METALS, 1998, 50 (5-6) :355-376
[5]   Stress development in alumina scales formed upon oxidation of (111)NiAl single crystals [J].
Lipkin, DM ;
Clarke, DR ;
Hollatz, M ;
Bobeth, M ;
Pompe, W .
CORROSION SCIENCE, 1997, 39 (02) :231-242
[6]   Measurement of the stress in oxide scales formed by oxidation of alumina-forming alloys [J].
Lipkin, DM ;
Clarke, DR .
OXIDATION OF METALS, 1996, 45 (3-4) :267-280
[7]   Characterization of a cyclic displacement instability for a thermally grown oxide in a thermal barrier system [J].
Mumm, DR ;
Evans, AG ;
Spitsberg, IT .
ACTA MATERIALIA, 2001, 49 (12) :2329-2340
[8]   Damage quantification in TBCs by photo-stimulated luminescence spectroscopy [J].
Nychka, JA ;
Clarke, DR .
SURFACE & COATINGS TECHNOLOGY, 2001, 146 :110-116
[9]   Piezospectroscopic analysis of interface debonding in thermal barrier coatings [J].
Peng, X ;
Clarke, DR .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2000, 83 (05) :1165-1170
[10]   High-temperature stress measurements during the oxidation of NiAl [J].
Schumann, E ;
Sarioglu, C ;
Blachere, JR ;
Pettit, FS ;
Meier, GH .
OXIDATION OF METALS, 2000, 53 (3-4) :259-272