Inorganic particle toughening II: toughening mechanisms of glass bead filled epoxies

被引:108
作者
Lee, J [1 ]
Yee, AF [1 ]
机构
[1] Univ Michigan, Macromol Sci & Engn Program, Ann Arbor, MI 48109 USA
基金
美国国家卫生研究院;
关键词
epoxy; fracture; toughening;
D O I
10.1016/S0032-3861(00)00398-0
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Based on the previously established knowledge about the micro-mechanical deformations occurring during the fracture of glass bead filled epoxies, the major energy dissipation mechanisms are investigated. Correlation studies between the fracture toughness of composites and the size of micro-mechanical deformation zones (or areal density of deformation) are used to assess the contributions of the deformations to toughening. Among the deformations found in the fracture of glass bead filled epoxies, i.e. micro-shear banding, debonding of glass beads/diffuse matrix shear yielding, and step formation, micro-shear banding is established as the major and most effective toughening mechanism. In terms of this mechanism, the negligible effect of surface treatments of glass beads on the fracture toughness of glass bead/thermoset composites can be explained successfully This mechanism is expected to give more detailed and fundamental understanding of inorganic particle toughening than the crack front bowing mechanism. (C) 2000 Published by Elsevier Science Ltd.
引用
收藏
页码:589 / 597
页数:9
相关论文
共 50 条
[1]   PLASTIC DEFORMATION BANDS IN GLASSY POLYSTYRENE [J].
ARGON, AS ;
ANDREWS, RD ;
GODRICK, JA ;
WHITNEY, W .
JOURNAL OF APPLIED PHYSICS, 1968, 39 (03) :1899-&
[2]   Fatigue of hybrid epoxy composites: Epoxies containing rubber and hollow glass spheres [J].
Azimi, HR ;
Pearson, RA ;
Hertzberg, RW .
POLYMER ENGINEERING AND SCIENCE, 1996, 36 (18) :2352-2365
[3]   FORMATION OF MICRO SHEAR BANDS IN POLYSTYRENE AND POLYMETHYLMETHACRYLATE [J].
BOWDEN, PB ;
RAHA, S .
PHILOSOPHICAL MAGAZINE, 1970, 22 (177) :463-+
[4]  
BOWDEN PB, 1970, PHILOS MAG, V25, P455
[5]   EFFECT OF INTERFACIAL BONDING ON TOUGHNESS OF GLASS FILLED POLYMERS [J].
BROUTMAN, LJ ;
SAHU, S .
MATERIALS SCIENCE AND ENGINEERING, 1971, 8 (02) :98-&
[6]  
BROWN SK, 1980, BR POLYM J, P24
[7]   CONTINUUM THEORY OF DILATANT TRANSFORMATION TOUGHENING IN CERAMICS [J].
BUDIANSKY, B ;
HUTCHINSON, JW ;
LAMBROPOULOS, JC .
INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 1983, 19 (04) :337-355
[8]   STRENGTH OF BRITTLE MATERIALS CONTAINING SECOND PHASE DISPERSIONS [J].
EVANS, AG .
PHILOSOPHICAL MAGAZINE, 1972, 26 (06) :1327-&
[9]   MECHANISMS OF TOUGHENING IN RUBBER TOUGHENED POLYMERS [J].
EVANS, AG ;
AHMAD, ZB ;
GILBERT, DG ;
BEAUMONT, PWR .
ACTA METALLURGICA, 1986, 34 (01) :79-87
[10]   ON THE TOUGHNESS OF PARTICULATE FILLED POLYMERS [J].
EVANS, AG ;
WILLIAMS, S ;
BEAUMONT, PWR .
JOURNAL OF MATERIALS SCIENCE, 1985, 20 (10) :3668-3674