Characterization and properties of a red and orange Y2O2S-based long afterglow phosphor

被引:185
作者
Wang, XX [1 ]
Zhang, ZT [1 ]
Tang, ZL [1 ]
Lin, YH [1 ]
机构
[1] Tsing Hua Univ, Dept Mat Sci & Engn, State Key Lab New Ceram & Fine Proc, Beijing 100084, Peoples R China
基金
中国国家自然科学基金;
关键词
luminescence; afterglow; red and orange phosphor; Y2O2S : Eu;
D O I
10.1016/S0254-0584(02)00097-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Eu3+-activated Y2O2S phosphors co-doped with Ti and Mg ions were prepared. The effect of various sintering atmospheric conditions on the crystalline phases and luminescent properties of the products were investigated in detail. Red and orange long afterglow was observed after phosphors were excited with 365 nm ultraviolet light. The main emission peaks were ascribed to Eu3+ ions transition from D-5(J) (J = 0, 1) to F-7(J) (J = 0, 1, 2, 3, 4), and the phosphorescence lasted for nearly 3 h in the light perception of the dark-adapted human eye (0.32 mcd m(-2)). The phosphorescence mechanism was also investigated. (C) 2002 Published by Elsevier Science B.V.
引用
收藏
页码:1 / 5
页数:5
相关论文
共 12 条
[1]  
[Anonymous], [No title captured]
[2]   GLOW CURVES WITH GENERAL ORDER KINETICS [J].
CHEN, R .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1969, 116 (09) :1254-&
[3]   MG2+ RELATED DEFECT CENTERS IN LIF-MG, TI [J].
HE, SS .
PHYSICA STATUS SOLIDI A-APPLIED RESEARCH, 1994, 144 (02) :K83-K86
[4]  
Katsumata T, 1998, J AM CERAM SOC, V81, P413, DOI 10.1111/j.1151-2916.1998.tb02349.x
[5]  
LIN Y, 1991, J EUR CERAM SOC, V21, P683
[6]   Synthesis of Eu3+-activated yttrium oxysulfide red phosphor by flux fusion method [J].
Lo, CL ;
Duh, JG ;
Chiou, BS ;
Peng, CC ;
Ozawa, L .
MATERIALS CHEMISTRY AND PHYSICS, 2001, 71 (02) :179-189
[7]   FLUORESCENT PROPERTIES OF ALKALINE EARTH ALUMINATES OF TYPE MAL204 ACTIVATED BY DIVALENT EURROPIUM [J].
PALILLA, FC ;
LEVINE, AK ;
TOMKUS, MR .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1968, 115 (06) :642-&
[8]  
PHANTHI M, 1991, J ELECTROCHEM SOC, V138, P1100
[9]   Long-lasting afterglow characteristics of Eu, Dy codoped SrO-Al2O3 phosphor [J].
Takasaki, H ;
Tanabe, S ;
Hanada, T .
JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1996, 104 (04) :322-326
[10]  
United States Patent Office, 1968, US Pat, Patent No. 3418246