Transient phenomena of the codeposition of PTFE with electroless Ni-P coating at the early stage

被引:27
作者
Ger, MD [1 ]
Hou, KH
Hwang, BJ
机构
[1] Natl Def Univ, Chung Cheng Inst Technol, Dept Appl Chem, Electrochem Microfabricat Lab, Tao Yuan 335, Taiwan
[2] Natl Def Univ, Chung Cheng Inst Technol, Dept Vehicle Engn, Tao Yuan 335, Taiwan
[3] Natl Taiwan Univ Sci & Technol, Dept Chem Engn, Microelectchem Lab, Taipei 106, Taiwan
关键词
Ni-P/PTFE; electroless; codeposition; surfactants;
D O I
10.1016/j.matchemphys.2004.05.004
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of surfactants on the transient phenomena of the codeposition of PTFE with electroless Ni-P coating at the early stage was investigated in this study. Two surfactants (CTAB and FC134) are utilized for comparison. The composition variation of the deposited layer is strongly related to the cathodic reactivity of the surfactants depending on the substrates at the early stage. When the cathodic reactivity of the surfactants is higher, correspondingly the PTFE particles are more easily embedded in the codeposition layer. The volume fraction of PTFE loading increases with the growth of the codeposition layer when the cathodic reactivity of surfactants on a substrate is less than that on the deposited layer. On the contrary, the volume fraction of PTFE loading decreases with the growth of the codeposition layer. Increasing the PTFE loading with the growth of the codeposition layer would provide good adhesion between the substrate and the codeposition layer. (C) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:102 / 108
页数:7
相关论文
共 13 条
[1]  
BARTLETT PKN, 1980, IND TRAINING REPORT, V10
[2]  
EBDON PR, 1988, PLAT SURF FINISH, V75, P65
[3]   ANALYSIS OF THE ELECTROLYTIC CODEPOSITION OF NON-BROWNIAN PARTICLES WITH METALS [J].
FRANSAER, J ;
CELIS, JP ;
ROOS, JR .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1992, 139 (02) :413-425
[4]   Effect of surfactants on codeposition of PTFE particles with electroless Ni-P coating [J].
Ger, MD ;
Hwang, BJ .
MATERIALS CHEMISTRY AND PHYSICS, 2002, 76 (01) :38-45
[5]   The friction and wear of Ni-P-PTFE composite deposits under water lubrication [J].
Ger, MD ;
Hou, KH ;
Wang, LM ;
Hwang, BJ .
MATERIALS CHEMISTRY AND PHYSICS, 2003, 77 (03) :755-764
[6]  
Ger MD, 2001, J CHIN INST CHEM ENG, V32, P503
[7]  
HADLEY JS, 1987, MET FINISH, V85, P51
[8]   Electrochemical deposition of zinc-polystyrene composites in the presence of surfactants [J].
Hovestad, A ;
Heesen, RJCHL ;
Janssen, LJJ .
JOURNAL OF APPLIED ELECTROCHEMISTRY, 1999, 29 (03) :331-338
[9]  
Hu X., 1997, PLAT SURF FINISH, V3, P51
[10]  
Matsuda H., 1994, Trans. Inst. Met. Finish., V72, P55, DOI [10.1080/00202967.1994.11871023, DOI 10.1080/00202967.1994.11871023]