Low-thermal-expansion copper composites via negative cte metallic elements

被引:31
作者
Mavoori H. [1 ,2 ,3 ,5 ,6 ]
Jin S. [3 ,4 ,5 ]
机构
[1] Appl. Mat. and Metall. Res. Group, Bell Laboratories, Lucent Technologies
[2] University of California, Berkeley, CA
[3] Bell Laboratories, Lucent Technologies
[4] Bell Laboratories, Murray Hill, NJ 07974
关键词
Thermomechanical Fatigue; Thermal Expansion Curve; Powder Metallurgy Approach; Complex Failure Mechanism; Thermal Management Design;
D O I
10.1007/s11837-998-0133-9
中图分类号
学科分类号
摘要
Thermal management is an important issue in electronic packaging due to the increasing complexity, miniaturization, and high density of components in modern devices. In high-power-dissipation packages, heat sinks are essential for preventing thermal damage to heat-sensitive components on the silicon chip. However, commonly used heat-sink materials (e.g., copper and aluminum alloys) have a much higher coefficient of thermal expansion (CTE) than silicon. CTE mismatch between the various materials in an electronic package can lead to stresses that can trigger complex failure mechanisms like component distortion, stress rupture, thermomechanical fatigue, and creep, thereby seriously degrading device reliability and lifetime. Therefore, it is highly desirable to minimize the CTE mismatch by developing new heat-sink materials having CTEs that are close to the CTE of silicon. In this work, low-thermal-expansion copper composites with CTEs as low as 4 ppm/°C have been fabricated by employing a negative thermalexpansion alloy - equiatomic Ni-Ti, which has a CTE of approximately -21 ppm/°C. The use of negative CTE elements, especially those with very large negative CTE values, offers an attractive route for controlling the thermal-expansion behavior of various metallic and nonmetallic materials.
引用
收藏
页码:70 / 72
页数:2
相关论文
共 12 条
[1]  
Shackelford J.F., CRC Materials Sci. and Eng. Hbk., 2nd Ed., (1992)
[2]  
Schmidt K.A., Zweben C., Electronic Materials Handbook, Vol. 1: Packaging, 1, (1989)
[3]  
Cottle C.D., Et al., JOM, 50, 6, (1998)
[4]  
Vaynman S., Et al., Proc. NEPCON West '96, (1996)
[5]  
Martinek C., Hummel F.A., J. Am. Ceram. Soc., 51, (1968)
[6]  
Mary T.A., Et al., Science, 272, (1996)
[7]  
Kowach G.R., Et al.
[8]  
Taylor D., J. British Ceram. Trans, 83, (1984)
[9]  
Mavoori H., Jin S.
[10]  
Jin S., Mavoori H., Tiefel T.H.