PVC films were degraded by outdoor exposure, irradiation by a weatherometer and heating by an electric oven. In PVC films subjected to outdoor exposure and to irradiation by the weatherometer at a low temperature, e. g. sample surface temperature of 0°C, photo‐oxidation and scission of the main chain were caused, but dehydrochlorination or formation of solvent‐insoluble substances were not observed. In contrast, PVC subjected to irradiation by the weatherometer at a high temperature, e. g. sample surface temperature of 80°C, showed a degradation tendency similar to that of PVC heated at 200°C in the electric oven, and decomposition of the thermal degradation type characterized by dehydrochlorination, formation of polyenes and formation of solvent‐insoluble substances were observed. © 1979 Hüthig & Wepf Verlag, Basel
引用
收藏
页码:113 / 122
页数:10
相关论文
共 11 条
[1]  
BASE SK, 1961, PAINT MANUF, V31, P345
[2]  
HIRT RC, 1967, MOD PLAST, V44, P156
[3]  
KARMAL MR, 1970, POLYM ENG SCI, V10, P108
[4]  
KARMAL MR, 1967, APPL POLYM S, V4, P1
[5]  
KUIST CH, 1968, PLAST ENG, V24, P46
[6]  
KURIHARA F, 1967, NIPPON GOMU KYOKAISH, V40, P648
[7]  
MARCHINOVICH RJ, 1967, APPL POLYM S, V4, P141
[8]  
MINEMATSU Y, 1972, PLASTICS, V23, P13
[9]   STUDIES ON PHOTODEGRADATION OF POLYVINYL-CHLORIDE) .1. [J].
MORI, F ;
KOYAMA, M ;
OKI, Y .
ANGEWANDTE MAKROMOLEKULARE CHEMIE, 1977, 64 (SEP) :89-99
[10]   STUDIES ON PHOTODEGRADATION OF POLYVINYL-CHLORIDE) .2. [J].
MORI, F ;
KOYAMA, M ;
OKI, Y .
ANGEWANDTE MAKROMOLEKULARE CHEMIE, 1978, 68 (MAY) :137-148