THE DISSOLUTION MECHANISMS OF SILICATE AND GLASS-IONOMER DENTAL CEMENTS

被引:64
作者
KUHN, AT
WILSON, AD
机构
关键词
D O I
10.1016/0142-9612(85)90096-1
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
引用
收藏
页码:378 / 382
页数:5
相关论文
共 36 条
[1]   INHIBITION OF NUCLEAR WASTE GLASS LEACHING BY CHEMISORPTION [J].
BUCKWALTER, CQ ;
PEDERSON, LR .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1982, 65 (09) :431-436
[2]   THE PHYSICO-MECHANICAL CONSEQUENCES OF EXPOSING GLASS IONOMER CEMENTS TO WATER DURING SETTING [J].
CAUSTON, BE .
BIOMATERIALS, 1981, 2 (02) :112-115
[3]   FACTORS RELATING TO THE RATE OF FLUORIDE-ION RELEASE FROM GLASS-IONOMER CEMENT [J].
CRANFIELD, M ;
KUHN, AT ;
WINTER, GB .
JOURNAL OF DENTISTRY, 1982, 10 (04) :333-341
[4]   GLASS IONOMER CEMENTS - CHEMISTRY OF EROSION [J].
CRISP, S ;
LEWIS, BG ;
WILSON, AD .
JOURNAL OF DENTAL RESEARCH, 1976, 55 (06) :1032-1041
[5]  
Crisp S, 1976, J Dent, V4, P162, DOI 10.1016/0300-5712(76)90025-7
[6]  
DAVIES EH, 1982, J MATER SCI, V17, P3263
[7]  
HEIMERL W, 1973, MANAGEMENT RADIOACTI, P536
[8]  
HORNSBY PR, 1977, THESIS BRUNEL U
[9]  
HURD DC, 1979, ACS SYM SER, V93, P413
[10]  
KENT BE, 1969 LAB GOV CHEM RE