STRIP EXTENSIOMETRY FOR COMPARISON OF THE MECHANICAL RESPONSE OF BOVINE, RABBIT, AND HUMAN CORNEAS

被引:202
作者
HOELTZEL, DA [1 ]
ALTMAN, P [1 ]
BUZARD, K [1 ]
CHOE, KI [1 ]
机构
[1] UNIV NEVADA,SCH MED,DEPT SURG,DIV OPHTHALMOL,LAS VEGAS,NV 89102
来源
JOURNAL OF BIOMECHANICAL ENGINEERING-TRANSACTIONS OF THE ASME | 1992年 / 114卷 / 02期
关键词
D O I
10.1115/1.2891373
中图分类号
Q6 [生物物理学];
学科分类号
071011 [生物物理学];
摘要
Specimens of bovine, rabbit, and human corneas were systematically tested in uniaxial tension to experimentally determine their effective nonlinear stress-strain relations, and hysteresis. Cyclic tensile tests were performed over the physiologic load range of the cornea, up to a maximum of 10 percent strain beyond slack strain. Dimensional changes to corneal test specimens, due to varying laboratory environmental conditions, were also assessed. The measured stress-strain data was found to closely fit exponential power function relations typical of collagenous tissues when appropriate account was taken of specimen slack strain. These constitutive relations are very similar for rabbit, human and bovine corneas, there was no significant difference between the species after preconditioning by one cycle. The uniaxial stress strain curves for all species behave similarly in that their tangent moduli increase at high loads and decrease at low loads as a function of cycling. In the bovine and rabbit data, there is a general trend towards more elastic behavior from the first to second cycles, but there is little variation in these parameters from the second to third cycles. In comparison, the human data demonstrates relatively little change between cycles. Increases in width of corneal test specimens, up to a maximum of 2 percent were found to occur under 95 percent relative humidity test conditions over 10 minutes elapsed time test periods, while specimens which were exposed to normal laboratory conditions (45 percent RH) were found to shrink in width up to a maximum of 9.5 percent over the same elapsed time period. The thickness of the test specimens were observed to decrease by 3 percent in 95 percent relative humidity and by 12 percent in 45 percent relative humidity over the same elapsed time period.
引用
收藏
页码:202 / 215
页数:14
相关论文
共 37 条
[1]
ACHENBAHC JD, 1974, COMPOSITE MATERIALS, V5, P313
[2]
BIOMECHANICAL PROPERTIES OF KERATOCONUS AND NORMAL CORNEAS [J].
ANDREASSEN, TT ;
SIMONSEN, AH ;
OXLUND, H .
EXPERIMENTAL EYE RESEARCH, 1980, 31 (04) :435-441
[3]
DEPENDENCE OF STRESS-STRAIN NONLINEARITY OF CONNECTIVE TISSUES ON GEOMETRY OF COLLAGEN-FIBERS [J].
COMNINOU, M ;
YANNAS, IV .
JOURNAL OF BIOMECHANICS, 1976, 9 (07) :427-433
[4]
CROXTON FE, 1959, ELEMENTARY STATISTIC, P235
[5]
DENHARTOG JP, 1987, ADV STRENGTH MATERIA, P70
[6]
EDMUND C, 1989, ACTA OPHTHALMOL, V67, P9
[7]
CROSS-SECTIONAL AREA MEASUREMENTS FOR TENDON SPECIMENS - A COMPARISON OF SEVERAL METHODS [J].
ELLIS, DG .
JOURNAL OF BIOMECHANICS, 1969, 2 (02) :175-&
[8]
OCULAR RIGIDITY IN KERATOCONUS [J].
FOSTER, CS ;
YAMAMOTO, GK .
AMERICAN JOURNAL OF OPHTHALMOLOGY, 1978, 86 (06) :802-806
[9]
FUNG YC, 1981, BIOMECHANICS
[10]
FUNG YC, 1987, AM J PHYSIOL, V213, P1532