POLARIZATION BEHAVIOR OF AUSTENITIC AND DUPLEX STAINLESS-STEELS IN THE DOUBLE LOOP REACTIVATION TEST

被引:20
作者
GOODWIN, SJ [1 ]
QUAYLE, B [1 ]
NOBLE, FW [1 ]
机构
[1] BRITISH NUCL FUELS,SELLAFIELD,CUMBRIA,ENGLAND
关键词
D O I
10.5006/1.3583863
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
引用
收藏
页码:743 / 747
页数:5
相关论文
共 20 条
[1]  
Akashi M., 1980, BOSHOKU GIJUTSU, V29, P163
[2]  
Borland J.C., 1960, BR WELD J, V7, P22
[3]  
BOWEN AW, 1975, MET T, V1, P1695
[4]   CHROMIUM DEPLETION AND MARTENSITE FORMATION AT GRAIN-BOUNDARIES IN SENSITIZED AUSTENITIC STAINLESS-STEEL [J].
BUTLER, EP ;
BURKE, MG .
ACTA METALLURGICA, 1986, 34 (03) :557-570
[5]   INFLUENCE OF CARBON CONTENT AND FERRITE MORPHOLOGY ON THE SENSITIZATION OF DUPLEX STAINLESS-STEEL [J].
DEVINE, TM .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1980, 11 (05) :791-800
[6]   MECHANISM OF INTERGRANULAR CORROSION AND PITTING CORROSION OF AUSTENITIC AND DUPLEX 308 STAINLESS-STEEL [J].
DEVINE, TM .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1979, 126 (03) :374-385
[7]  
EDMONDS DP, 1978, PROPERTIES STEEL WEL, P47
[8]   PHASE-TRANSFORMATION AND IMPACT PROPERTIES OF TYPE 17-8-2 AUSTENITIC WELD METALS [J].
FARRAR, RA ;
HUELIN, C ;
THOMAS, RG .
JOURNAL OF MATERIALS SCIENCE, 1985, 20 (08) :2828-2838
[9]  
FARRAR RA, 1985, J MATER SCI, V18, P3461
[10]  
GILL TPS, 1982, J MATER SCI, V17, P1513, DOI 10.1007/BF00752268