PREPARATION OF FINE NI PARTICLES BY THE SPRAY-PYROLYSIS TECHNIQUE AND THEIR FILM FORMING PROPERTIES IN THE THICK-FILM METHOD

被引:44
作者
NAGASHIMA, K
WADA, M
KATO, A
机构
[1] Department of Applied Chemistry, Faculty of Engineering, Kyushu University, Higashiku, Fukuoka 812
关键词
D O I
10.1557/JMR.1990.2828
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fine Ni particles were directly prepared from Ni(N03)2and NiCl2 aqueous solutions by the spray-pyrolysis technique under an H2-N2atmosphere. Hollow Ni particles with rough surfaces were obtained at a low reaction temperature (700–900 °C). With increasing reaction temperatures from 900 °C to 1500 °C, the particles varied gradually to solid ones with a smooth surface, and the particles obtained at 1600 °C were perfectly spherical ones whose average size was —0.6 μm. From the point of view that aggregation free powders are considered to be good for thick film applications, Ni(N03)2was preferred to NiCl2as a starting material. The perfectly spherical particles derived from Ni(N03)2gave a Ni film about 3 μm in thickness having sheet resistance of 37.7 mΩ square-1. © 1990, Materials Research Society. All rights reserved.
引用
收藏
页码:2828 / 2834
页数:7
相关论文
共 10 条
  • [1] HIRATA Y, 1984, MEM FAC ENG KAGOSHIM, V20, P73
  • [2] KATO A, 1985, J CHEM SOC JPN, P2342
  • [3] NAGASHIMA K, IN PRESS J MATER SCI
  • [4] NAGASHIMA K, 1987, J CHEM SOC JPN, P2293
  • [5] NAGASHIMA K, 1989, J JPN SOC POWDER POW, V36, P278
  • [6] NAGASHIMA K, 1990, J CHEM SOC JPN, V17
  • [7] RANG RJ, 1962, J ACOUST SOC AM, V34, P6
  • [8] SPROSON DW, 1987, ADV CERAM, V21, P99
  • [9] TUNODA S, 1987, ELECTRONIC CERAMICS, V18, P33
  • [10] 1987, Patent No. 6202404