POLYMER DEGRADATION DURING COMBUSTION

被引:10
作者
BRAUMAN, SK [1 ]
机构
[1] SRI INT,MENLO PK,CA 94025
关键词
D O I
10.1002/polb.1988.090260602
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
引用
收藏
页码:1159 / 1171
页数:13
相关论文
共 17 条
[1]   ANALYSIS OF NONVOLATILE OXIDATION PRODUCTS OF POLYPROPYLENE .1. THERMAL OXIDATION [J].
ADAMS, JH .
JOURNAL OF POLYMER SCIENCE PART A-1-POLYMER CHEMISTRY, 1970, 8 (05) :1077-&
[2]   POLYSTYRENE DEGRADATION DURING COMBUSTION [J].
BRAUMAN, SK ;
CHEN, IJ ;
MATZINGER, DP .
JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 1983, 21 (06) :1831-1845
[3]  
BRAUMAN SK, 1977, J FIRE RETARD CHEM, V4, P38
[4]  
BRAUMAN SK, 1981, J FIRE RETARD CHEM, V8, P8
[5]  
BRAUMAN SK, 1976, J FIRE RETARD CHEM, V3, P138
[6]  
BRAUMAN SK, 1977, J FIRE FLAMMABILITY, V8, P210
[7]   THERMAL AND OXIDATIVE-DEGRADATION OF POLY(METHYL METHACRYLATE) - WEIGHT-LOSS [J].
HIRATA, T ;
KASHIWAGI, T ;
BROWN, JE .
MACROMOLECULES, 1985, 18 (07) :1410-1418
[8]  
JELLINEK HH, 1968, MAKROMOL CHEM, V115, P89
[9]   THERMAL AND OXIDATIVE-DEGRADATION OF POLY(METHYL METHACRYLATE) - MOLECULAR-WEIGHT [J].
KASHIWAGI, T ;
HIRATA, T ;
BROWN, JE .
MACROMOLECULES, 1985, 18 (02) :131-138
[10]  
KASHIWAGI T, 1986, 1ST FIR SAF SCI P IN, P483