THERMAL AND ELECTRICAL RESISTIVITIES OF RHENIUM FROM 2 DEGREES K TO 20 DEGREES K

被引:24
作者
SCHRIEMP.JT
机构
关键词
D O I
10.1016/0022-3697(67)90045-5
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
引用
收藏
页码:2581 / +
页数:1
相关论文
共 12 条
[1]   INTERBAND ELECTRON-ELECTRON SCATTERING AND TRANSPORT PHENOMENA IN SEMICONDUCTORS [J].
APPEL, J .
PHYSICAL REVIEW, 1962, 125 (06) :1815-&
[2]   EFFECT OF ELECTRON-ELECTRON SCATTERING ON ELECTRICAL AND THERMAL CONDUCTIVITY OF METALS [J].
APPEL, J .
PHILOSOPHICAL MAGAZINE, 1963, 8 (90) :1071-&
[3]   PROPERTIES OF GOLD + 0.03 PER CENT ( AT ) IRON THERMOELEMENTS BETWEEN 1 + 300 DEGREES K + BEHAVIOUR IN MAGNETIC FIELD [J].
BERMAN, R ;
BROCK, JCF ;
HUNTLEY, DJ .
CRYOGENICS, 1964, 4 (04) :233-&
[4]  
BERMAN R, 1963, CRYOGENICS, V3, P70
[6]  
MENDELSSOHN K, 1961, SOLID STATE PHYS, V12, P223
[7]  
Plumb H., 1966, METROLOGIA, V2, P127, DOI DOI 10.1088/0026-1394/2/4/001
[8]   LOW TEMPERATURE THERMOELECTRIC POWER OF GOLD-IRON VERSUS SILVER NORMAL THERMOCOUPLES [J].
SCHRIEMPF, JT ;
SCHINDLER, AI .
CRYOGENICS, 1966, 6 (05) :301-+
[9]   A COMPARISON OF EQUATIONS FOR GERMANIUM RESISTOR THERMOMETRY IN 2-20DEGREES K RANGE [J].
SCHRIEMPF, JT .
CRYOGENICS, 1966, 6 (06) :362-+
[10]   PREPARATION OF HIGH-PURITY RHENIUM SINGLE CRYSTALS [J].
SODEN, RR ;
BRENNERT, GF ;
BUEHLER, E .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1965, 112 (01) :77-&