FRACTURE-TOUGHNESS AND FLEXURAL STRENGTH OF DENTAL CERAMICS FOR TITANIUM

被引:25
作者
KVAM, K
DERAND, T
AUSTRHEIM, EK
机构
[1] NIOM, Scandinavian Institute of Dental Materials, Haslum
关键词
CERAMICS; DENTAL MATERIALS; FLEXURAL STRENGTH; FRACTURE TOUGHNESS; TITANIUM;
D O I
10.1016/0142-9612(95)91099-K
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Three brands of dental ceramics for veneering to titanium: TitanBond (O'Hara), Ti-Ceram (Ducera) and Titankeramik (Vita) were tested to compare their fracture properties in wet and in dry conditions. Eight polished and precracked specimens of each material were stored in water at 37 degrees C for 28 d and then preloaded in a four-point bending jig with a constant load of 50 N for 24 h under water. Five of the specimens were fractured by a four-point bending test also under water at 37 degrees C. Crack depths were measured in three different positions in each of the remaining three specimens. Fracture load and crack depths were used to calculate the fracture toughness. Another ten polished specimens were used to measure the flexural strength with a four-point Pending test after storage in water at 37 degrees C for 28 d. Equal procedures and numbers of specimens were used to measure fracture toughness and flexural strength without preloading and storage in water.
引用
收藏
页码:73 / 76
页数:4
相关论文
共 11 条
[1]  
[Anonymous], 1972, ADV INORG CHEM
[2]  
BINNS D, 1983, DENTAL CERAMICS, P58
[3]  
DIETER GE, 1976, MECHANICAL METALLURG, P259
[4]  
DUNCAN RV, 1980, ENG DESIGN GUIDES, V39, P8
[5]  
JONES DW, 1983, DENTAL CERAMICS, P110
[6]  
KRAUSE RF, 1984, ASTM STP, V855, P309
[7]   FRACTURE-TOUGHNESS DETERMINATION OF CERAMIC AND RESIN-BASED DENTAL COMPOSITES [J].
KVAM, K .
BIOMATERIALS, 1992, 13 (02) :101-104
[8]   FRACTURE-TOUGHNESS OF COMMERCIAL DENTAL PORCELAINS [J].
MORENA, R ;
LOCKWOOD, PE ;
FAIRHURST, CW .
DENTAL MATERIALS, 1986, 2 (02) :58-62
[9]  
NORUSIS MJ, 1986, SPSS PC PLUS IBM PC
[10]  
RICHERSON DW, 1982, MODERN CERAMIC ENG, P86