FRACTURE-BEHAVIOR OF W-NI-FE HEAVY ALLOYS

被引:123
作者
CHURN, KS [1 ]
GERMAN, RM [1 ]
机构
[1] RENSSELAER POLYTECH INST, DEPT MAT ENGN, TROY, NY 12181 USA
来源
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 1984年 / 15卷 / 02期
关键词
POWDER METALLURGY - Tungsten;
D O I
10.1007/BF02645119
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The compositions ranged from 93 to 97 wt pct W, with the Ni:Fe ratio maintained at 7:3. Room temperature strength and ductility showed degradation with sintering times in access of two hours. Initial cracking occurs at the tungsten-tungsten grain boundaries and in the tungsten grain. These latter cracks propagate to give eventual failure. The ductility to failure is governed by the strength of the tungsten-matrix interface. The maximum elongation depends on the contiguity which in turn is set by composition.
引用
收藏
页码:331 / 338
页数:8
相关论文
共 46 条
[1]  
ANDERSON PB, 1967, PLANSEEBER PULVERMET, V15, P180
[2]  
Bazhenova L. G., 1980, Soviet Powder Metallurgy and Metal Ceramics, V19, P34
[3]  
Bukatov V. G., 1982, Soviet Powder Metallurgy and Metal Ceramics, V21, P785, DOI 10.1007/BF00795885
[4]  
CHERMANT JL, 1979, POWDER METALL INT, V11, P106
[5]   FRACTURE TOUGHNESS AND FRACTURE OF WC-CO COMPOSITES [J].
CHERMANT, JL ;
OSTERSTOCK, F .
JOURNAL OF MATERIALS SCIENCE, 1976, 11 (10) :1939-1951
[6]  
Cherniavsky K. S., 1982, Science of Sintering, V14, P1
[7]   PORE FORMATION AND ITS EFFECT ON MECHANICAL-PROPERTIES IN W-NI-FE HEAVY ALLOY [J].
CHURN, KS ;
YOON, DN .
POWDER METALLURGY, 1979, 22 (04) :175-178
[8]  
EBKOM L, 1976, SCAND J METALL, V5, P179
[9]   INTERFACIAL EMBRITTLEMENT IN LIQUID-PHASE SINTERED TUNGSTEN HEAVY ALLOYS [J].
EDMONDS, DV ;
JONES, PN .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1979, 10 (03) :289-295
[10]  
EISENMANN MR, 1982, PROG POWDER MET, V38, P203