RAPIDLY SOLIDIFIED AL3TI-BASE ALLOYS CONTAINING NI

被引:46
作者
HUANG, SC [1 ]
HALL, EL [1 ]
GIGLIOTTI, MFX [1 ]
机构
[1] GE,CORP RES & DEV,SCHENECTADY,NY 12301
关键词
D O I
10.1557/JMR.1988.0001
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
引用
收藏
页码:1 / 7
页数:7
相关论文
共 20 条
  • [1] IMPROVEMENT IN ROOM-TEMPERATURE DUCTILITY OF THE L12 TYPE INTERMETALLIC COMPOUND NI3A1 BY BORON ADDITION
    AOKI, K
    IZUMI, O
    [J]. JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1979, 43 (12) : 1190 - 1196
  • [2] Davies H.A., 1980, 2ND P INT C RAP SOL, P153
  • [3] HORI S, 1973, J JPN I METALL, V37, P1135
  • [4] RAPID SOLIDIFICATION CHARACTERISTICS IN MELT SPINNING A NI-BASE SUPERALLOY
    HUANG, SC
    LAFORCE, RP
    RITTER, AM
    GOEHNER, RP
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1985, 16 (10): : 1773 - 1779
  • [5] BORON EXTENDED SOLUBILITY AND STRENGTHENING POTENCY IN RAPIDLY SOLIDIFIED NI3AL
    HUANG, SC
    TAUB, AI
    CHANG, KM
    [J]. ACTA METALLURGICA, 1984, 32 (10): : 1703 - 1707
  • [6] HUANG SC, 1986, 1986 P MAT RES SOC S, V2, P481
  • [7] INOUE A, 1980, 1980 P INT C TIT KYO, P1137
  • [8] KEAR BH, 1962, T METALL SOC AIME, V224, P382
  • [9] EFFECT OF BORON ON GRAIN-BOUNDARIES IN NI3AL
    LIU, CT
    WHITE, CL
    HORTON, JA
    [J]. ACTA METALLURGICA, 1985, 33 (02): : 213 - 229
  • [10] MARKIV VY, 1973, AKAD NAUK UKR SSSR M, V46, P103