SYNTHESIS AND CHARACTERIZATION OF ALPHA,OMEGA-BIS(4-HYDROXYBUTYL) POLYDIMETHYLSILOXANES

被引:16
作者
LAI, YC
OZARK, R
QUINN, ET
机构
[1] Bausch & Lomb Inc., Rochester, New York
关键词
HYDROXY-TERMINATED POLYSILOXANE; SYNTHESIS; CHARACTERIZATION; MOLECULAR WEIGHT DETERMINATION; STABILITY;
D O I
10.1002/pola.1995.080331104
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
alpha,omega-Bis(4-hydroxybutyl) polydimethylsiloxane (molecular weight 1500 to 4500) can be prepared with well-controlled molecular weight through the reaction of 1,3-bis(4-hydroxybutyl)tetramethyl disiloxane and dimethoxydimethyl silane or diethoxydimethyl silane in the presence of a stoichiometric amount of water and hydrochloric acid. The molecular weight of these hydroxybutyl-terminated polysiloxanes can be determined fairly consistently by a titration method. These polysiloxanes are stable toward cyclization. (C) 1995 John Wiley and Sons, Inc.
引用
收藏
页码:1773 / 1782
页数:10
相关论文
共 9 条
[1]  
KOJIMA K, 1969, J POLYM SCI, V4, P2325
[2]   SYNTHESIS AND STRUCTURE PROPERTY RELATIONSHIPS OF UV-CURABLE URETHANE PREPOLYMERS WITH HARD-SOFT HARD BLOCKS [J].
LAI, YC ;
BACCEI, LJ .
JOURNAL OF APPLIED POLYMER SCIENCE, 1991, 42 (07) :2039-2044
[3]   NOVEL POLYURETHANE SILICONE HYDROGELS [J].
LAI, YC .
JOURNAL OF APPLIED POLYMER SCIENCE, 1995, 56 (03) :301-310
[4]   SYNTHESES AND CHARACTERIZATION OF UV-CURABLE POLYSILOXANE-BASED POLYURETHANE PREPOLYMERS [J].
LAI, YC ;
QUINN, ET .
JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 1995, 33 (11) :1783-1793
[5]  
NOSHAY A, 1977, BLOCK COPOLYMERS
[6]  
SORENSEN WR, 1968, PREPARATIVE METHOD P, P43
[7]  
STECKLE WP, 1987, ACS POLYM PREPR, V28, P264
[8]   POLY(CHLOROPROPYLMETHYL-DIMETHYLSILOXANE)-POLYURETHANE ELASTOMERS - SYNTHESIS AND PROPERTIES OF SEGMENTED COPOLYMERS AND RELATED ZWITTERIONOMERS [J].
YU, X ;
NAGARAJAN, MR ;
LI, C ;
GIBSON, PE ;
COOPER, SL .
JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 1986, 24 (12) :2681-2702
[9]  
1987, SILICONE COMPOUNDS R, P262