MODE-II STRESS INTENSITY FACTORS FOR A CRACK PARALLEL TO THE SURFACE OF AN ELASTIC HALF-SPACE SUBJECTED TO A MOVING POINT LOAD

被引:109
作者
HEARLE, AD
JOHNSON, KL
机构
[1] Univ of Cambridge, Dep of, Engineering, Cambridge, Engl, Univ of Cambridge, Dep of Engineering, Cambridge, Engl
关键词
ELASTICITY - MATERIALS - Crack Propagation - STRESSES;
D O I
10.1016/0022-5096(85)90022-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The direction of propagation of rolling contact fatigue cracks is observed to depend upon the direction of motion of the load. In this paper approximate calculations are described of the variation of Mode II stress intensity factors at each tip of a subsurface crack, which lies parallel to the surface of an elastic half-space, due to a load moving over the surface. In particular the effect of frictional locking of the crack faces under the load is investigated. In consequence of frictional locking the range of SIF at the trailing tip DELTA K//T is found to be about 30% greater than that of the leading tip DELTA K//L, which is consistent with observations that subsurface cracks propagate predominantly in the direction of motion of the load over the surface. The effects of K//T and K//L of crack length, crack face friction, traction forces at the surface and residual shear stresses are also investigated.
引用
收藏
页码:61 / &
相关论文
共 15 条
[1]  
CHANG FK, 1984, UNPUB J APPL MECH
[2]   MECHANICS OF CRACK-PROPAGATION IN DELAMINATION WEAR [J].
FLEMING, JR ;
SUH, NP .
WEAR, 1977, 44 (01) :39-56
[3]  
HAHN GT, 1984, UNPUB 6 INT C FRACT
[4]  
HEARLE AD, 1983, CMECHTR26 CAMBR U EN
[5]   APPLICATION OF FRACTURE-MECHANICS TO WEAR [J].
HILLS, DA ;
ASHELBY, DW .
WEAR, 1979, 54 (02) :321-330
[6]   ON THE DETERMINATION OF STRESS INTENSIFICATION FACTORS FOR A WEARING HALF-SPACE [J].
HILLS, DA ;
ASHELBY, DW .
ENGINEERING FRACTURE MECHANICS, 1980, 13 (01) :69-&
[7]  
MCCLINTOCK FA, 1977, 4 INT C FRACT, V4, P23
[8]  
MERWIN JE, 1963, P I MECH ENG, V177, P667
[9]  
OREGAN SD, 1984, UNPUB WEAR
[10]  
PONTER ARS, 1984, UNPUB J MECH PHYS SO