The subject of improving the fracture toughness of fibre composites is receiving significant attention because a critical design criterion in damage tolerant fibre composites is the possession of a sufficiently high fracture energy absorption capability, particularly under impact loading conditions. For a given brittle-fibre/brittle-matrix composite, high strength requires a strong interfacial bond, but this may lead to a low fracture energy absorption. However, by proper control of the physical and mechanical properties of the fibre-matrix interface high strength characteristics can be combined with high toughness. In order to fully utilise the potential of such composites without introducing a reduction in strength, it is necessary to understand the failure mechanisms leading to eventual fracture. This paper reviews the existing theories of fracture toughness of fibre composites and the various methods for improving the fracture toughness by means of interface control. Conclusions and generalisations which can be drawn from the literature are presented with discussions of areas in which further research is required.
引用
收藏
页码:333 / 378
页数:46
相关论文
共 234 条
[1]  
Almond E.A., 1969, ASTM STP, V452, P107
[2]  
ANDONIAN R, 1979, INT J CEM COMPOSITES, V2, P151
[3]   A NEW COUPLING AGENT FOR ARAMID FIBERS [J].
ANDREOPOULOS, AG .
JOURNAL OF APPLIED POLYMER SCIENCE, 1989, 38 (06) :1053-1064
[4]  
[Anonymous], ASTM STP
[5]  
ANSTICE PD, 1981, P ICF 5, V1, P473
[6]   EFFECT OF INTERLAYERS ON TRANSVERSE STRESSES IN FIBER COMPOSITES [J].
ARRIDGE, RGC .
POLYMER ENGINEERING AND SCIENCE, 1975, 15 (10) :757-760
[7]  
ASHBY MF, 1989, ACTA METALL, V37, P1237
[8]   INTERMITTENT BONDING FOR HIGH TOUGHNESS - HIGH-STRENGTH COMPOSITES [J].
ATKINS, AG .
JOURNAL OF MATERIALS SCIENCE, 1975, 10 (05) :819-832
[9]   IMPARTING STRENGTH AND TOUGHNESS TO BRITTLE COMPOSITES [J].
ATKINS, AG .
NATURE, 1974, 252 (5479) :116-118
[10]   EFFECT OF WATER AND ICE ON STRENGTH AND FRACTURE TOUGHNESS OF INTERMITTENTLY BONDED BORON-EPOXY COMPOSITES [J].
ATKINS, AG ;
MAI, YW .
JOURNAL OF MATERIALS SCIENCE, 1976, 11 (12) :2297-2306