IMPROVED HEAT-RESISTANCE OF MG-AL ALLOYS BY THE CA ADDITION

被引:287
作者
NINOMIYA, R
OJIRO, T
KUBOTA, K
机构
[1] R and D Center, Mitsui Mining and Smelting Co. Ltd. Haraichi 1333-2, Ageo, Saitama
来源
ACTA METALLURGICA ET MATERIALIA | 1995年 / 43卷 / 02期
关键词
D O I
10.1016/0956-7151(94)00269-N
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The addition of Ca into Mg-(3-9)wt%Al alloys increased the hardness at the high temperatures up to 350 degrees C. In particular, this was remarkable when the mass ratio of Ca to Al was higher than 0.8, probably owing to the precipitation of the Mg,Ca phase in the alloys. Such alloys with the Ca/Al mass ratio higher than 0.8 showed excellent heat resistance at a moderate temperature. Therefore, they were considered to be the new promising light-weight heat-resistant alloys for interior automotive applications.
引用
收藏
页码:669 / 674
页数:6
相关论文
共 11 条
[1]  
BASNER TG, 1993, 930419 SAE TECH PAP
[2]  
CATTERALL JA, 1957, J I MET, V86, P189
[3]  
HECTOR B, 1989, INGEIEUR WERKSTOFFE, V5, P62
[4]  
HECTOR B, 1990, 900798 SAE TECH PAP
[5]  
HOLLRIGL-ROSTA F, 1980, LIGHT MET AGE, V38, P22
[6]  
KAWASE Y, 1991, 910549 SAE TECH PAP
[7]  
MASSALSKI TB, 1986, BINARY ALLOY PHASE D, V1, P129
[8]  
MERCER WE, 1990, 900788 SAE TECH PAP
[9]  
NINOMIYA R, IN PRESS J JAPAN I L
[10]  
PENNINGTONS JN, 1990, MODERN METALS, P113