STRESS-CORROSION CRACKING INITIATION IN FERRITIC STAINLESS-STEELS IN A CHLORIDE ENVIRONMENT

被引:14
作者
LOCCI, IE
KWON, HK
HEHEMANN, RF
TROIANO, AR
机构
关键词
D O I
10.5006/1.3583886
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
引用
收藏
页码:465 / 470