STRESS WHITENING IN POLYETHYLENE

被引:29
作者
CHERRY, BW
HIN, TS
机构
关键词
D O I
10.1016/0032-3861(81)90372-4
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
引用
收藏
页码:1610 / 1612
页数:3
相关论文
共 12 条
[1]  
BENHAM PP, 1971, PLAST POLYM, V39, P130
[2]  
BREUER H, 1977, J MACROMOL SCI PHYS, VB14, P387, DOI 10.1080/00222347708212908
[3]   ENERGY-RELATED FAILURE CRITERIA OF THERMOPLASTICS [J].
BRULLER, OS .
POLYMER ENGINEERING AND SCIENCE, 1981, 21 (03) :145-150
[4]  
CARMICHAEL AJ, 1964, AUST J APPL SCI, V15, P389
[5]   SUPERSTRUCTURE OF HIGH-DENSITY POLYETHYLENE FILM CRYSTALLIZED FROM STRESSED POLYMER MELTS AS OBSERVED BY SMALL-ANGLE LIGHT-SCATTERING [J].
HASHIMOTO, T ;
NAGATOSHI, K ;
TODO, A ;
KAWAI, H .
POLYMER, 1976, 17 (12) :1075-1085
[6]   ULTRAHIGH MODULUS POLYETHYLENE .2. EFFECT OF DRAWING TEMPERATURE ON VOID FORMATION AND MODULUS [J].
JARECKI, L ;
MEIER, DJ .
JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 1979, 17 (09) :1611-1621
[7]  
KAMBOUR RP, 1973, MACROMOL REV, V7, P136
[8]   MACROSCOPIC VOLUME CHANGES OF SELECTED POLYMERS SUBJECTED TO UNIFORM TENSILE DEFORMATION [J].
POWERS, JM ;
CADDELL, RM .
POLYMER ENGINEERING AND SCIENCE, 1972, 12 (06) :432-&
[9]  
REINER M, 1964, FRACTURE PROCESSES P
[10]  
VINCENT PI, 1973, 2ND INT C YIELD DEF