The objective of the present work has been to extend the sol-gel method of obtaining pure mullite to mullite-ZrO//2 composites with 15 to 20 vol% of ZrO//2 for strengthening and toughening and to investigate the densification and retention of tetragonal ZrO//2 in the matrix of synthetic mullite.