共 53 条
[1]
[Anonymous], METALLURGICAL REV
[2]
FORMATION OF CAVITIES FROM NON-DEFORMABLE 2ND-PHASE PARTICLES IN LOW-TEMPERATURE DUCTILE FRACTURE
[J].
JOURNAL OF ENGINEERING MATERIALS AND TECHNOLOGY-TRANSACTIONS OF THE ASME,
1976, 98 (01)
:60-68
[3]
DISTRIBUTION OF PLASTIC STRAIN AND NEGATIVE-PRESSURE IN NECKED STEEL AND COPPER BARS
[J].
METALLURGICAL TRANSACTIONS,
1975, A 6 (04)
:815-824
[4]
SEPARATION OF SECOND-PHASE PARTICLES IN SPHEROIDIZED 1045 STEEL, CU-0.6PCT CR ALLOY, AND MARAGING-STEEL IN PLASTIC STRAINING
[J].
METALLURGICAL TRANSACTIONS,
1975, A 6 (04)
:839-851
[5]
BACKOFEN WA, 1964, FRACTURE ENGINEERING, P107
[6]
Barsom J. M., 1973, Engineering Fracture Mechanics, V5, P209, DOI 10.1016/0013-7944(73)90018-0
[7]
BROWN LM, 1973, P 3 INT C STRENGTH M, V1, P164
[8]
CHERMANT JL, 1979, J MATER SCI, V14, P509
[9]
ROLE OF HYDROGEN IN THE DUCTILE FRACTURE OF PLAIN CARBON-STEELS
[J].
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE,
1979, 10 (03)
:367-375
[10]
INVESTIGATION OF PLASTIC FRACTURE OF ALSL-4340 AND 18 NICKEL-200 GRAE MARAGING STEELS
[J].
METALLURGICAL TRANSACTIONS,
1974, 5 (06)
:1457-1470