UNLUBRICATED SLIDING WEAR OF CERAMICS AGAINST GRAPHITIZED CAST IRONS

被引:23
作者
FANG, L
GAO, YM
ZHOU, L
LI, P
机构
[1] Department of Mechanical Engineering, Xian Jiaotong University, Xian
关键词
D O I
10.1016/0043-1648(94)90355-7
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Unlubricated sliding wear tests of Al2O3, Si3N4 and ZrO2 against ductile iron and grey cast iron were carried out on a ring-block wear tester at room temperature. It was found that the wear volume of ceramics increased in the order Al2O3, ZrO2, Si3N4. The wear volume of grey iron was greater than that of ductile iron. Energy-dispersive X-ray analyses of worn surfaces of the ceramics indicated that a large amount of cast iron formed a transfer layer on Al2O3, making the wear volume of Al2O3 the smallest among the three ceramics. The graphite in the cast irons can decrease the wear of the ceramic-cast iron pairs.
引用
收藏
页码:129 / 134
页数:6
相关论文
共 8 条
[1]   MULTILABORATORY TRIBOTESTING - RESULTS FROM THE VERSAILLES ADVANCED MATERIALS AND STANDARDS PROGRAM ON WEAR TEST METHODS [J].
CZICHOS, H ;
BECKER, S ;
LEXOW, J .
WEAR, 1987, 114 (01) :109-130
[2]   INTERNATIONAL MULTILABORATORY SLIDING WEAR TESTS WITH CERAMICS AND STEEL [J].
CZICHOS, H ;
BECKER, S ;
LEXOW, J .
WEAR, 1989, 135 (01) :171-191
[3]   THE FORMATION OF ALUMINUM HYDROXIDE IN THE SLIDING WEAR OF ALUMINA [J].
GEE, MG .
WEAR, 1992, 153 (01) :201-227
[4]  
JAHANMIR S, 1989, MATER RES SOC S P, V140, P285
[5]   EROSION OF HARD MATERIAL COATING SYSTEMS [J].
LEVY, AV ;
WANG, BQ .
WEAR, 1988, 121 (03) :325-346
[6]   WEAR TESTS OF GREY CAST-IRON AGAINST CERAMICS [J].
NAKAMURA, Y ;
HIRAYAMA, S .
WEAR, 1989, 132 (02) :337-345
[7]  
TSUNAI Y, 1989, P INT C WEAR MATERIA, P369
[8]  
ZHOU L, 1992, 2ND NATL C HEAT TREA, P35