CERAMIC-MATRIX COMPOSITE-METAL BRAZED JOINTS

被引:18
作者
DIXON, DG
机构
[1] British Aerospace PLC, Sowerby Research Centre FPC 267, Filton, BS12 7QW, Bristol
关键词
D O I
10.1007/BF00375261
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A silicon nitride fibre-reinforced cordierite glass ceramic matrix composite has been brazed to titanium and stainless steel in argon with four different interlayer materials, copper, nickel, tungsten and a metal matrix composite (mmc). Joints were tested in shear and all but one failed in the ceramic composite. The highest strength joint, using a metal matrix interlayer to join cmc to stainless steel failed in the mmc at 106 MPa. Silver-copper eutectic braze and aluminium braze can be used to join metals to titanium-coated cmc, producing joints with low levels of interfacial defects. Some joints, however, show debonding at the edges where residual shear stresses are highest.
引用
收藏
页码:1539 / 1544
页数:6
相关论文
共 4 条
[1]  
DOYAMA M, 1979, METAL CERAMIC JOINTS
[2]  
LOEHMAN RE, 1988, AM CERAM SOC BULL, V67, P375
[3]  
NICHOLAS MG, 1986, BRIT CERAM TRANS J, V85, P144
[4]  
SANTELLA ML, 1988, ADV CERAM MATER, V3, P457