摘要
The mechanism underlying the rapid, early, capacity loss of titanium-based (Ti2Ni) hydrogen-storage alloys is examined via X-ray diffraction analysis. The formation and accumulation of Ti2NiH0.5, a hydride phase that cannot be reversibly charged/ discharged according to the experimental results, is proposed as a dominant cause of the early capacity loss of such electrodes.
引用
收藏
页码:101 / 106
页数:6
相关论文
共 5 条
[1]   LOW-TEMPERATURE SURFACE MICRO-ENCAPSULATION OF TI2NI HYDROGEN-STORAGE ALLOY POWDERS [J].
LUAN, B ;
CUI, N ;
LIU, HK ;
ZHAO, H ;
DOU, SX .
JOURNAL OF POWER SOURCES, 1994, 52 (02) :295-299
[2]  
MARKIN TL, 1981, J ELECTROANAL CHEM, V118, P211
[3]   EFFECTS OF MICROENCAPSULATION OF HYDROGEN STORAGE ALLOY ON THE PERFORMANCES OF SEALED NICKEL METAL HYDRIDE BATTERIES [J].
SAKAI, T ;
ISHIKAWA, H ;
OGURO, K ;
IWAKURA, C ;
YONEYAMA, H .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1987, 134 (03) :558-562
[4]   THE SYSTEM LANI5-H2 [J].
SHILOV, AL ;
KOST, ME ;
KUZNETSOV, NT .
JOURNAL OF THE LESS-COMMON METALS, 1988, 144 (01) :23-30
[5]   FROM PERMANENT-MAGNETS TO RECHARGEABLE HYDRIDE ELECTRODES [J].
WILLEMS, JJG ;
BUSCHOW, KHJ .
JOURNAL OF THE LESS-COMMON METALS, 1987, 129 :13-30