3-YEAR OCCLUSAL WEAR OF POSTERIOR COMPOSITE RESTORATIONS

被引:23
作者
FREILICH, MA
GOLDBERG, AJ
GILPATRICK, RO
SIMONSEN, RJ
机构
[1] UNIV TENNESSEE CTR HLTH SCI,COLL DENT,DEPT GEN DENT,MEMPHIS,TN 38163
[2] THREE M CO,HLTH CARE,US & INT DENT PROD DIV,ST PAUL,MN 55144
关键词
D O I
10.1016/0109-5641(92)90089-U
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
The specific aims of this study were to: 1) measure the occlusal wear of four different dental composite materials placed in the posterior teeth of adults; and 2) evaluate the effect of the clinical parameters, cavity class and tooth type on occlusal wear. Four different visible light-cured composite materials were used to make the restorations in this study. The restorations placed for this randomized clinical trial were scored through the use of an indirect evaluation system (M-L scale). The total sample size per recall ranged from 90 to 142 restorations from baseline to 36 months. The mean wear at 36 months for Heliomolar, J&J Experimental (Adaptic II) and P-30 was 45 - 54 mum, which is rather low compared to the recently reported wear of other composite materials. Marathon exhibited significantly greater wear with a mean of 174 mum at 36 months. The data also showed that cavity class and tooth type had no significant effect on the occlusal wear of the restorations made with the three low wear-rate materials, while restorations composed of the high wear-rate material exhibited more wear in molars than premolars; this effect was again not statistically significant. These data support the hypothesis that the overall wear of a composite restoration is more dependent on the material's properties than clinical parameters such as cavity class and tooth type.
引用
收藏
页码:224 / 228
页数:5
相关论文
共 19 条
[1]  
BAYNE S C, 1991, Journal of Dental Research, V70, P344
[2]   A VISIBLE LIGHT-CURED POSTERIOR COMPOSITE RESIN - RESULTS OF A 3-YEAR CLINICAL-EVALUATION [J].
BOKSMAN, L ;
JORDAN, RE ;
SUZUKI, M ;
CHARLES, DH .
JOURNAL OF THE AMERICAN DENTAL ASSOCIATION, 1986, 112 (05) :627-631
[3]   DIRECT AND INDIRECT EVALUATION OF POSTERIOR COMPOSITE RESTORATIONS AT 3 YEARS [J].
FREILICH, MA ;
GOLDBERG, AJ ;
GILPATRICK, RO ;
SIMONSEN, RJ .
DENTAL MATERIALS, 1992, 8 (01) :60-64
[4]   CLINICAL-EVALUATION METHODS FOR POSTERIOR COMPOSITE RESTORATIONS [J].
GOLDBERG, AJ ;
RYDINGE, E ;
SANTUCCI, EA ;
RACZ, WB .
JOURNAL OF DENTAL RESEARCH, 1984, 63 (12) :1387-1391
[5]   WEAR RATES OF POSTERIOR COMPOSITE RESINS [J].
LEINFELDER, KF ;
WILDER, AD ;
TEIXEIRA, LC .
JOURNAL OF THE AMERICAN DENTAL ASSOCIATION, 1986, 112 (06) :829-833
[6]   USING COMPOSITE RESIN AS A POSTERIOR RESTORATIVE MATERIAL [J].
LEINFELDER, KF .
JOURNAL OF THE AMERICAN DENTAL ASSOCIATION, 1991, 122 (04) :65-70
[7]   QUANTITATIVE WEAR MEASUREMENT OF POSTERIOR COMPOSITE RESINS [J].
LEINFELDER, KF ;
TAYLOR, DF ;
BARKMEIER, WW ;
GOLDBERG, AJ .
DENTAL MATERIALS, 1986, 2 (05) :198-201
[8]  
LEINFELDER KF, 1988, CLIN RESTORATIVE MAT, P87
[9]  
Lugassy AA, 1985, J DENT RES, V64, P181
[10]  
LUNDIN SA, 1989, SWED DENT J, V13, P217