The wear characteristics of sintered diamond composite segmented sawblades during circular sawing of granite were investigated. Scanning electron microscopy, optical microscopy and energy-dispersive X-ray analysis were used to identify wear mechanisms. The forces acting on the blade for various sawblades were also measured. The results obtained show that fracture of diamond particles can be attributed to impact forces and low cyclic surface fatigue, and wear of the matrix bond is due to flush erosion, cavitation erosion and abrasion. Blades containing diamonds with a greater degree of etching pits result in a relatively higher proportion of macro-fractured or polished (flattened) diamond particles, a larger vertical sawing force and sawing force ratio, and lower grinding ratio than those containing diamonds covered with less etching pits.
引用
收藏
页码:325 / 337
页数:13
相关论文
共 12 条
[1]  
BAILEY MW, 1979, IND DIAMOND REV, V39, P56
[2]  
BURGESS RR, 1978, 30TH ANN M SEM IND D
[3]  
Buttner A., 1974, IND DIAMOND REV, V34, P89
[4]   WEAR OF DIAMOND [J].
CROMPTON, D ;
HIRST, W ;
HOWSE, MGW .
PROCEEDINGS OF THE ROYAL SOCIETY OF LONDON SERIES A-MATHEMATICAL AND PHYSICAL SCIENCES, 1973, 333 (1595) :435-+
[5]  
ERTINGSHAUSEN W, 1985, IND DIAMOND REV, V45, P254
[6]  
MAMALIS AG, 1979, IND DIAMOND REV, V39, P356
[7]  
T?nshoff, 1986, ANN CIRP, V35, P239, DOI [10.1016/S0007-8506(07)61879-4, DOI 10.1016/S0007-8506(07)61879-4]
[8]  
Tnshoff H. K., 1982, ADV ULTRAHARD MAT AP, V1, P36
[9]  
TOKURA H, 1989, J MATER SCI, V24, P2232
[10]  
WILKS J, 1979, PROPERTIES DIAMOND, P351