FRACTURE-BEHAVIOR OF ORIENTED POLY(ETHER-ETHER-KETONE) (PEEK)

被引:10
作者
WU, GM [1 ]
SCHULTZ, JM [1 ]
机构
[1] UNIV DELAWARE,MAT SCI PROGRAM,NEWARK,DE 19716
关键词
D O I
10.1002/pen.760290609
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
引用
收藏
页码:405 / 414
页数:10
相关论文
共 22 条
[1]   SYNTHESIS AND PROPERTIES OF POLYARYLETHERKETONES [J].
ATTWOOD, TE ;
DAWSON, PC ;
FREEMAN, JL ;
HOY, LRJ ;
ROSE, JB ;
STANILAND, PA .
POLYMER, 1981, 22 (08) :1096-1103
[2]  
BLUNDELL DJ, 1986, SAMPE QUART, V17, P50
[3]  
BLUNDELL DJ, 1985, SAMPE QUART, V17, P1
[4]  
Broek D., 1986, ELEMENTARY ENG FRACT
[5]   EFFECT OF PRE-ORIENTATION ON FRACTURE PROPERTIES OF GLASSY POLYMERS [J].
CURTIS, JW .
JOURNAL OF PHYSICS D-APPLIED PHYSICS, 1970, 3 (10) :1413-&
[6]   EFFECT OF SHORT FIBER REINFORCEMENT ON THE FATIGUE CRACK-PROPAGATION AND FRACTURE OF PEEK-MATRIX COMPOSITES [J].
FRIEDRICH, K ;
WALTER, R ;
VOSS, H ;
KARGERKOCSIS, J .
COMPOSITES, 1986, 17 (03) :205-216
[7]  
HARTNESS JT, 1983, SAMPE QUART, V14, P33
[8]  
HAY JN, 1984, POLYM COMMUN, V25, P175
[9]   TEMPERATURE AND STRAIN-RATE EFFECTS ON THE FRACTURE-TOUGHNESS OF POLY(ETHER ETHER KETONE) AND ITS SHORT GLASS-FIBER REINFORCED COMPOSITE [J].
KARGERKOCSIS, J ;
FRIEDRICH, K .
POLYMER, 1986, 27 (11) :1753-1760
[10]   THE MICROSTRUCTURE OF INJECTION-MOLDED SEMI-CRYSTALLINE POLYMERS - A REVIEW [J].
KATTI, SS ;
SCHULTZ, JM .
POLYMER ENGINEERING AND SCIENCE, 1982, 22 (16) :1001-1017