IR STUDIES OF WOOD PLASTIC COMPOSITES

被引:52
作者
KHAN, MA [1 ]
ALI, KMI [1 ]
BASU, SC [1 ]
机构
[1] UNIV DHAKA,DEPT CHEM,DHAKA 1000,BANGLADESH
关键词
D O I
10.1002/app.1993.070490905
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Wood plastic composites (WPC) of simul were prepared by gamma radiation using butylacrylate (BA) and methylmethacrylate (MMA) as the monomer and methanol as the swelling agent at 9:1 (v/v) ratio. IR spectra of simul, bulk polymer of BA (or MMA) film, and WPC of different polymer loadings ranging from 18 to 115% were studied. Increase of the characteristic peak intensity at 1735 cm-1 (C=0 vibration for acetyl groups) over that of 1620 cm-1 (conjugated aryl carbonyl groups) along with the increase of polymer loading of simul with the monomer indicates that the graft copolymerization took place between the monomer and the simul wood matrix. (C) 1993 John Wiley & Sons, Inc.
引用
收藏
页码:1547 / 1551
页数:5
相关论文
共 7 条
[1]  
CHOW SZ, 1972, WOOD SCI, V5, P27
[2]  
KHAN MA, 1991, RADIAT PHYS CHEM, V38, P303
[3]  
KHAN MA, 1992, RADIAT PHYS CHEM, V40, P69
[4]  
KHAN MA, 1991, RADIAT PHYS CHEM, V38, P537
[5]  
Marchessault R.H., 1962, PURE APPL CHEM, V5, P107, DOI DOI 10.1351/PAC196205010107
[6]  
YAP MGS, 1992, J APPL POLYM SCI, V43, P2083
[7]  
YAP MGS, 1979, CAD J CHEM, V57, P2603