The title compounds were synthesized by sintering mixtures of fine metal powders at optimized experimental conditions of temperature (450-500-degrees-C) and hydrogen pressure (90 bar). In contrast to previous work, nearly single-phase samples of up to 10 g were obtained in a single-step process.