COMPARATIVE FRACTOGRAPHY OF CHEMICAL VAPOR AND COMBUSTION DEPOSITED DIAMOND FILMS

被引:12
作者
HOFF, HA
MORRISH, AA
BUTLER, JE
RATH, BB
机构
[1] Naval Research Laboratory, Washington
关键词
D O I
10.1557/JMR.1990.2572
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Polycrystalline diamond films of several thicknesses have been fractured by manual bending and examined by scanning electron microscopy. These films have been deposited in controlled environments at low pressures by chemical vapor deposition and in ambient atmosphere with an oxygen-acetylene torch. Fracture surfaces in the low pressure depositions exhibit cleavage steps across the grains. These surfaces, independent of thickness, are primarily transgranular, attesting to the inherent strength of the deposits. However, the ambient deposited diamond has primarily intergranular fracture indicative of weak grain boundaries. Internal defects, observed with transmission electron microscopy, such as twins, stacking faults, and dislocations, occur generally in both types of deposition with no apparent preference for location or type of deposition. © 1990, Materials Research Society. All rights reserved.
引用
收藏
页码:2572 / 2588
页数:17
相关论文
共 23 条
[1]   LOW-PRESSURE, METASTABLE GROWTH OF DIAMOND AND DIAMONDLIKE PHASES [J].
ANGUS, JC ;
HAYMAN, CC .
SCIENCE, 1988, 241 (4868) :913-921
[2]  
BUTLER JE, 1990, IN PRESS HIGH TEMP S
[3]   DIAMOND GROWTH IN O-2 + C2H4 AND O2 + C2H2 FLAMES [J].
CARRINGTON, WA ;
HANSSEN, LM ;
SNAIL, KA ;
OAKES, DB ;
BUTLER, JE .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1989, 20 (07) :1282-1284
[4]  
DEVRIES RC, 1987, ANNU REV MATER SCI, V17, P161
[5]  
DUNN KJ, 1979, J MATER SCI, V14, P882
[6]  
FREITAS JA, 1989, MATER RES SOC S P, V162
[7]  
GIGL PD, 1979, HIGH PRESSURE SCI TE, V1, P914
[8]   DIAMOND SYNTHESIS USING AN OXYGEN-ACETYLENE TORCH [J].
HANSSEN, LM ;
CARRINGTON, WA ;
BUTLER, JE ;
SNAIL, KA .
MATERIALS LETTERS, 1988, 7 (7-8) :289-292
[9]  
HANSSEN LM, 1990, IN PRESS J APPL PHYS
[10]  
HOFF HA, 1990, IN PRESS CERAM T