Mechanical properties and adhesion strength of TiN and Al coatings on HSS, steel, aluminium and copper characterized by four testing Methods

被引:16
作者
Muller, D
Fromm, E
机构
[1] Max-Planck-Institut für Metallforschung, Institut für Werkstoffwissenschaft, D-70174 Stuttgart
关键词
adhesion; titanium nitride; aluminium; copper; steel;
D O I
10.1016/0040-6090(95)06931-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
TiN and Al coatings on substrates of high-speed steel, steel, aluminium and copper have been used to study mechanical properties of coating systems, especially the adhesion of the coating. The quantities measured are internal stress of the coating, determined by X-ray diffraction, the critical load of the scratch test, the microhardness obtained by the indenter technique, and the interface fracture energy, determined by a three-point bend test developed recently by the authors. The fracture energy, G(c), is a measure for the adhesion strength of a coating system, The effect of bias voltage, sputter cleaning and contamination of the substrates on the adhesion strength and other mechanical properties are investigated with the four methods mentioned. Each of the testing methods reveal only specific aspects of the behaviour of the coating systems. The data obtained depend on bulk properties of the film and the substrate material and on properties of the interface. Variation of the bias voltage can change them in quite different ways. In addition, the inter-relations between the adhesion strength of the coating and the failure behaviour of the three-point bend test samples are discussed.
引用
收藏
页码:411 / 416
页数:6
相关论文
共 20 条
[1]   EFFECT OF CONTAMINATION REACTIONS ON THE COMPOSITION AND MECHANICAL-PROPERTIES OF MAGNETRON SPUTTERED TIN COATINGS [J].
BERG, S ;
EGUCHI, N ;
GRAJEWSKI, V ;
KIM, SW ;
FROMM, E .
SURFACE & COATINGS TECHNOLOGY, 1991, 49 (1-3) :336-341
[2]   EFFECT OF CONTAMINATION ON MECHANICAL-PROPERTIES AND ADHESION OF MAGNETRON-SPUTTERED TIN COATINGS ON HIGH-SPEED STEEL SUBSTRATES [J].
BERG, S ;
KIM, SW ;
GRAJEWSKI, V ;
FROMM, E .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1991, 139 :345-351
[3]  
COTTERELL B, 1965, INT J FRACT MECH, V1, P96
[4]  
DREIER G, 1993, EINFLUSS THERMISCHER, V18
[5]   SPUTTER CLEANING OF IRON SUBSTRATES AND CONTAMINATION OF TIN COATINGS STUDIED BY INSITU AUGER-ELECTRON SPECTROSCOPY MEASUREMENTS IN AN ULTRAHIGH-VACUUM PHYSICAL VAPOR-DEPOSITION APPARATUS [J].
EGUCHI, N ;
GRAJEWSKI, V ;
UCHIDA, HH ;
FROMM, E .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1991, 139 :339-344
[6]  
ELSSNER G, 1985, J PHYSIQUE C, V4, P597
[7]  
EVANS AG, 1989, ACTA METALL MATER, V37, P917
[8]  
JAYATILAKA AD, 1979, FRACTURE ENG BRITTLE, P91
[9]   REVISED STRUCTURE ZONE MODEL FOR THIN-FILM PHYSICAL STRUCTURE [J].
MESSIER, R ;
GIRI, AP ;
ROY, RA .
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 1984, 2 (02) :500-503
[10]  
MITTAL KL, 1978, STP AM SOC TESTING M, V640, P7