HIGH-TEMPERATURE CORROSION IN SOFC ENVIRONMENTS

被引:133
作者
KOFSTAD, P [1 ]
BREDESEN, R [1 ]
机构
[1] CTR IND RES,N-0314 OSLO 3,NORWAY
关键词
D O I
10.1016/0167-2738(92)90092-4
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The corrosive environment in solid oxide fuels cells (SOFCs) using natural gas (mainly methane) as fuel is considered. In the anode chamber the gas is highly carburizing at the gas inlet and after gradual oxidation it becomes highly humid, but weakly oxidizing (high CO2:CO ratio) at the gas outlet; in the cathode chamber the gas is highly oxidizing (air). In addition to noble metals, nickel and chromia-forming alloys are considered as potential metallic interconnects and their corrosion behaviour in the SOFC environment is discussed.
引用
收藏
页码:69 / 75
页数:7
相关论文
共 14 条
[1]  
ANDERSON HU, 1989, P ELECTROCHEM SOC, V8911, P111
[2]  
Betteridge W., 1984, NICKEL ITS ALLOYS
[3]  
FANDEL M, 1990, 1ST P EUR CER SOC C, V2, P236
[4]   MICROSTRUCTURE, ADHESION AND GROWTH-KINETICS OF PROTECTIVE SCALES ON METALS AND ALLOYS [J].
HINDAM, H ;
WHITTLE, DP .
OXIDATION OF METALS, 1982, 18 (5-6) :245-284
[5]   LOCALIZED LEVEL HOPPING TRANSPORT IN LA(SR)CRO3 [J].
KARIM, DP ;
ALDRED, AT .
PHYSICAL REVIEW B, 1979, 20 (06) :2255-2263
[6]  
Kofstad P., 1988, HIGH TEMPERATURE OXI
[7]  
Kofstad P, 1972, NONSTOICHIOMETRY DIF, DOI DOI 10.1002/MACO.19740251027
[8]  
Kubaschewski O., 1967, METALLURGICAL THERMO
[9]   HIGH-TEMPERATURE OXIDATION OF FE-13CR-XAL ALLOYS IN AIR-H2O VAPOR MIXTURES [J].
KVERNES, I ;
OLIVEIRA, M ;
KOFSTAD, P .
CORROSION SCIENCE, 1977, 17 (03) :237-252
[10]   DEFECT STRUCTURE, IONIC-CONDUCTIVITY, AND DIFFUSION IN YTTRIA STABILIZED ZIRCONIA AND RELATED OXIDE ELECTROLYTES WITH FLUORITE STRUCTURE [J].
NAKAMURA, A ;
WAGNER, JB .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1986, 133 (08) :1542-1548