MECHANICAL-PROPERTIES OF 3 COMPOSITE RESINS FOR THE INLAY ONLAY TECHNIQUE

被引:26
作者
PEUTZFELDT, A
ASMUSSEN, E
机构
[1] Royal Dental College, Copenhagen
基金
英国医学研究理事会;
关键词
D O I
10.1016/0022-3913(91)90257-W
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
The present study measured the diametral compressive strength, flexural strength, and modulus of elasticity of composite resins used in inlay/onlay systems. The effect of additional curing also was determined. SR-Isosit material had the highest diametral compressive strength, and SR-Isosit-Dentin material had the lowest flexural strength. The SR-Isosit composite resins had lowest elastic modulus and Estilux posterior C VS resin the highest. A negative correlation was found between diametral compressive strength and elastic modulus of the materials. It was concluded that the additional curing of Brilliant resin did not result in improved mechanical properties. For Estilux resin, additional curing increased flexural strength and modulus of elasticity.
引用
收藏
页码:322 / 324
页数:3
相关论文
共 11 条
[1]  
ASMUSSEN E, 1990, SCAND J DENT RES, V98, P564
[2]  
ASMUSSEN E, 1982, SCAND J DENT RES, V90, P484
[3]   THE INFLUENCE OF TEMPERATURE ON SOME PHYSICAL-PROPERTIES OF DENTAL COMPOSITES [J].
BAUSCH, JR ;
DELANGE, C ;
DAVIDSON, CL .
JOURNAL OF ORAL REHABILITATION, 1981, 8 (04) :309-317
[4]  
FULLEMANN J, 1986, THESIS ZURICH
[5]  
HALD A, 1952, STATISTICAL THEORY E
[6]  
KAYE GW, 1959, TABLES PHYSICAL CHEM
[7]  
KULLMANN W, 1988, DEUT ZAHNAERZTL Z, V43, P383
[8]  
Lutz F, 1987, Phillip J Restaur Zahnmed, V4, P127
[9]  
REINHARDT KJ, 1988, DEUT ZAHNAERZTL Z, V43, P909
[10]  
Smith D, 1985, POSTERIOR COMPOSITE, P47