共 11 条
[1]
ALBRECHT J, 1976, 4TH P INT C STRENGTH, P403
[2]
DAHMEN U, 1975, Z METALLKD, V66, P255
[3]
HAHN GT, AF3361571C1915 TECH
[4]
HORNBOGEN E, 1977, ACTA MET, V25
[5]
DUCTILE FRACTURE IN INTERIOR OF PRECIPITATE FREE ZONE IN AN AL-6.0-PERCENT ZN-2.6-PERCENT MG ALLOY
[J].
ACTA METALLURGICA,
1976, 24 (09)
:817-825
[6]
MARTIN JC, TO BE PUBLISHED
[7]
NEUMANN P, 1967, Z METALLKD, V58, P781
[8]
RYUM N, 1967, Z METALLKD, V58, P28
[9]
ORIGIN OF BRITTLE INTERGRANULAR FATIGUE FRACTURE IN WARM AGED AL-3.6 WT PCT CU
[J].
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE,
1976, 7 (04)
:601-604
[10]
THOMAS G, 1959, J I MET, V88, P81