DAMAGE THRESHOLDS AT METAL-SURFACES FOR SHORT PULSE IR LASERS

被引:35
作者
FIGUEIRA, JF
THOMAS, SJ
机构
关键词
D O I
10.1109/JQE.1982.1071704
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
引用
收藏
页码:1381 / 1386
页数:6
相关论文
共 16 条
[1]  
BORN M, PRINCIPLES OPTICS, P615
[2]  
Carslaw H. S., 1959, CONDUCTION HEAT SOLI, P75
[3]   ALUMINUM MIRRORS AL2O3-PROTECTED, WITH HIGH REFLECTANCE AT NORMAL BUT GREATLY DECREASED REFLECTANCE AT HIGHER ANGLES OF INCIDENCE IN 8-12-MUM REGION [J].
COX, JT ;
HASS, G .
APPLIED OPTICS, 1978, 17 (03) :333-334
[4]   CARBON-DIOXIDE LASER SYSTEM WITH ZERO SMALL-SIGNAL GAIN [J].
FIGUEIRA, JF ;
NOWAK, AV .
APPLIED OPTICS, 1980, 19 (03) :420-421
[5]  
FIGUEIRA JF, 1982, APPL PHYS LETT, V40, P260
[6]  
GOLDSTEIN I, 1976, NBS SPECIAL PUBLICAT, V435
[7]  
HAYDEN JJ, 1977, NBS PUBLICATION, V462, P173
[8]  
MUMOLA PB, UNPUB P INT C LASERS
[9]  
NEWNAM BE, 1979, OPT ENG NOV, P579
[10]  
PORTEUS JO, 1980, NBS SPECIAL PUBLIC N, V568, P175