摘要
The use of commercially available and laboratory made Ni-Si-Cr brazes for wetting and bonding Si3N4 has been explored. The microstructure and chemistry of brazed joints has been characterized by techniques such as optical microscopy, scanning electron microscopy, electron probe micro-analysis and X-ray diffraction. Si3N4 was wetted well by all the braze alloys at 1150-1200 degrees C, but the joint quality obtained was poor because of the formation of brittle phases and solid solutions.
引用
收藏
页码:563 / 572
页数:10
相关论文
共 26 条
[1]  
ANSARA I, 1985, EUR96571EN COMM EUR
[2]  
FOLEY AG, 1993, 2ND P EUR C DES CER, P411
[3]  
Frisk K, 1990, THESIS ROYAL I TECHN
[4]  
GUPTA KP, 1969, T TMS AIME, V218, P617
[5]  
HADIAN AM, 1991, CERAM T, V19, P221
[6]  
HOLMSTROM M, 1992, 4TH INTERNATIONAL SYMPOSIUM ON CERAMIC MATERIALS AND COMPONENTS FOR ENGINES, P364
[7]  
Iida T., 1988, PHYSICAL PROPERTIES, P217
[8]  
IWAMOTO N, 1993, 2ND P EUR C DES CER, P441
[9]  
KODENTSOV A, IN PRESS
[10]  
KODENTSOV AA, 1993, CERAM T, V35, P13516