摘要
Seven 35% solids, (83 : 17 in mol %), vinylidene chloride (VDC)-butyl methacrylate (BMA) copolymer latexes were prepared at 25-degrees-C using redox catalyst by batch and seeded semicontinuous emulsion copolymerization processes: one batch (G), one seeded batch (F), and five seeded semicontinuous polymerizations of five different nonomer feed rates ranging from 0.27 (A) to 1.10 (E) wt % / min. All of the emulsion polymerizations gave stable latexes of almost 100% conversion with negligible coagulum and narrow particle size distributions. The kinetic studies of seeded semicontinuous polymerization A-E showed that the rates of polymerization (R(p)) were controlled by the monomer addition rates (R(a)), and polymerizations A-D (0.27-0.79 wt % / min) were under monomer-starved conditions; polymerization E (1.10 wt % / min) was in near-flooded condition. Significant differences were found in the physical and mechanical properties of the latex films, depending on the mode of monomer addition. Infrared spectroscopy, C-13 solid-state NMR spectroscopy, X-ray diffraction, the T(g) and T(m) values by DSC, dynamic mechanical spectroscopy, and tensile strength measurement of the latex films post-heat-treated for 30 min at 70-degrees-C or aged for several months at room temperature demonstrated that batch polymerizations F and G gave copolymers of heterogeneous composition and a crystalline character. In contrast, semicontinuous polymerizations A-E gave copolymers of more uniform composition and an amorphous character.
引用
收藏
页码:3133 / 3145
页数:13
相关论文
共 19 条
[1]  
BOVEY FA, 1982, CHAIN STRUCTURE CONF, pCH8
[2]  
CHUJO K, 1969, J POLYM SCI POL SYM, P321
[3]  
COBLER JG, 1972, POLYM THIN FILMS, P706
[4]   BATCH AND SEMICONTINUOUS EMULSION CO-POLYMERIZATION OF VINYL-ACETATE BUTYL ACRYLATE .1. BULK, SURFACE, AND COLLOIDAL PROPERTIES OF CO-POLYMER LATEXES [J].
ELAASSER, MS ;
MAKGAWINATA, T ;
VANDERHOFF, JW ;
PICHOT, C .
JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 1983, 21 (08) :2363-2382
[5]  
KOMOROSKI RA, 1984, P VINYLIDENE CHLORID
[6]   INFRARED SPECTRA OF HIGH POLYMERS .4. POLYVINYL CHLORIDE, POLYVINYLIDENE CHLORIDE, AND COPOLYMERS [J].
KRIMM, S ;
LIANG, CY .
JOURNAL OF POLYMER SCIENCE, 1956, 22 (100) :95-112
[7]  
LEE KC, 1987, THESIS LEHIGH U
[8]  
LUSKIN LS, 1967, ENCY IND CHEM ANAL, V4, P161
[9]  
MANSON JA, 1976, POLYM BLENDS COMPOSI, P412
[10]   EFFECT OF EMULSION POLYMERIZATION PROCESS ON THE MORPHOLOGY OF VINYL ACETATE-BUTYL ACRYLATE COPOLYMER LATEX FILMS [J].
MISRA, SC ;
PICHOT, C ;
ELAASSER, MS ;
VANDERHOFF, JW .
JOURNAL OF POLYMER SCIENCE PART C-POLYMER LETTERS, 1979, 17 (09) :567-572