ALLOYING AND POST-HEAT-TREATMENT OF THERMAL-SPRAYED COATINGS OF SELF-FLUXING ALLOYS

被引:26
作者
SHIEH, YH [1 ]
WANG, JT [1 ]
SHIH, HC [1 ]
WU, ST [1 ]
机构
[1] NATL TSING HUA UNIV,DEPT MAT SCI & ENGN,HSINCHU 300,TAIWAN
关键词
D O I
10.1016/0257-8972(93)90176-O
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The hardness and wear resistance of a thermal-sprayed self-fluxing alloy (Ni-17wt.%Cr-3.3wt.%B-4.3wt.%Si-4.2wt.%Fe-0.9wt.%C) is improved by adding 20 wt.% of B13C2 to the powder and heating the coating at 1030-degrees-C in a vacuum of 10(-2) Torr. Porosity is decreased from 20 to 0.3 vol.% by the heating if a pre-heating at 950-degrees-C is carried out to facilitate the escape of trapped gases. The presence of numerous precipitates of Cr3C2, and CrB in the coating is consistent with a Rockwell hardness of HRC 63. The abrasive wear resistance is much improved compared with that of Stellite 6B.
引用
收藏
页码:73 / 77
页数:5
相关论文
共 14 条
[1]  
BAKER JW, 1976, 8TH P INT THERM SPRA, P159
[2]   SINTERING ATMOSPHERE EFFECTS ON TENSILE PROPERTIES OF HEAVY ALLOYS [J].
BOSE, A ;
GERMAN, RM .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1988, 19 (10) :2467-2476
[3]  
Budinski KG., 1988, SURFACE ENG WEAR RES, V1
[4]  
CLARK WP, 1985, WELD J, V64, P69
[5]   SINTERING TIME AND ATMOSPHERE INFLUENCES ON THE MICROSTRUCTURE AND MECHANICAL-PROPERTIES OF TUNGSTEN HEAVY ALLOYS [J].
GERMAN, RM ;
BOSE, A ;
MANI, SS .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1992, 23 (01) :211-219
[6]   SINTERING ATMOSPHERE EFFECTS ON THE DUCTILITY OF W-NI-FE HEAVY-METALS [J].
GERMAN, RM ;
CHURN, KS .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1984, 15 (04) :747-754
[7]   STRUCTURE OF NI-CR-B-SI HARDFACING ALLOYS AND THEIR BONDING REACTIONS [J].
KNOTEK, O ;
LUGSCHEIDER, E .
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY, 1974, 11 (04) :798-801
[8]   PRESSURELESS SINTERING AND RELATED REACTION PHENOMENA OF AL2O3-DOPED B4C [J].
LEE, CH ;
KIM, CH .
JOURNAL OF MATERIALS SCIENCE, 1992, 27 (23) :6335-6340
[9]   VOLUME-DIFFUSION-CONTROLLED FINAL-STAGE DENSIFICATION OF A POROUS SOLID [J].
MARKWORTH, AJ .
SCRIPTA METALLURGICA, 1972, 6 (10) :957-+
[10]   SELF-FLUXING COATINGS FOR STATIONARY GAS-TURBINES [J].
NICOLL, AR .
THIN SOLID FILMS, 1982, 95 (03) :285-295