Thermal expansion and forced volume magnetostriction have been measured for Fe-Pt alloys containing 28-32 at% Pt. Values of the spontaneous volume magnetostriction at 0 K are found to be as large as those in Fe-Ni Invar alloys, while the forced volume magnetostriction at 4.2 K is about one order smaller than observed for Fe-Ni Invar alloys.