The most susceptible site for pit initiation was the retained delta ferrite/austenite interface. Microanalysis results disprove the chromium depletion theory. The most likely explanation is a segregation of impurities such as sulfur or phosphorus to the interface during the nonequilibrium solidification process associated with weldments. The passive film over the interface as well as repassivation kinetics are degraded by impurities.
引用
收藏
页码:246 / 251
页数:6
相关论文
共 25 条
[1]  
Arata Y., 1976, T JWRI, V5, P135
[2]   ANODIC POLARIZATION OF AUSTENITIC STAINLESS STEELS IN CHLORIDE MEDIA [J].
BOND, AP ;
LIZLOVS, EA .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1968, 115 (11) :1130-&
[3]  
BRITTON SC, 1932, J IRON ST I, V126, P365
[4]  
Forchhammer V. P., 1969, MATER CORROS, V20, P1, DOI [10.1002/maco.19690200103, DOI 10.1002/MACO.19690200103]
[5]  
GARNER A, 1978, MAR CORR 78 NAT ASS
[6]  
HOAR TP, 1953, J APPL CHEM, V3, P502
[7]  
HOAR TP, 1936, J IRON STEEL I, V133, P239
[8]  
LIPPOLD J, 1978, THESIS RENSSELAER PO
[9]  
LYMAN CE, 1978, SCANNING ELECTRON MI, V1, P213
[10]   EFFECT OF TEST METHOD AND SURFACE CONDITION ON PITTING POTENTIAL OF SINGLE AND DUPLEX PHASE 304L STAINLESS-STEEL [J].
MANNING, PE ;
DUQUETTE, DJ ;
SAVAGE, WF .
CORROSION, 1979, 35 (04) :151-157