EFFECT OF HEAT-TREATMENT ON DELAYED HYDRIDE CRACKING IN ZR-2.5 WT PCT NB

被引:26
作者
AMOUZOUVI, KF
CLEGG, LJ
机构
来源
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 1987年 / 18卷 / 10期
关键词
D O I
10.1007/BF02646200
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
引用
收藏
页码:1687 / 1694
页数:8
相关论文
共 30 条
[11]  
DUTTON R, 1978, HYDROGEN METALS, V1, P1
[12]  
DUTTON R, 1976, EFFECT HYDROGEN BEHA, P516
[13]  
DUTTON R, 1978, CAN MET Q, V17, P16
[14]  
LEGER M, 1985, CAN METALL QUART, V24, P235
[15]  
MAYER P, 1977, HYDROGEN METALS, V2, P1
[16]  
MISHIMA Y, 1971, METALL TRANS, V2, P1995
[17]  
Norwood D.O., 1983, INT METALS REV, V28, P92
[18]   HYDRIDE PRECIPITATION IN ALPHA-BETA-ZIRCONIUM ALLOYS [J].
PEROVIC, V ;
WEATHERLY, GC ;
SIMPSON, CJ .
ACTA METALLURGICA, 1983, 31 (09) :1381-1391
[19]  
PERRYMAN ECW, 1978, NUCL ENERG-J BR NUCL, V17, P95
[20]   THE EFFECTS OF MISFIT AND EXTERNAL STRESSES ON TERMINAL SOLID SOLUBILITY IN HYDRIDE-FORMING METALS [J].
PULS, MP .
ACTA METALLURGICA, 1981, 29 (12) :1961-1968