共 16 条
[11]
SOME OBSERVATIONS ON MICROSTRUCTURAL DAMAGE PRODUCED BY FATIGUE OF AN ALUMINIUM-7.5 PERCENT ZINC-2.5 PERCENT MAGNESIUM ALLOY AT TEMPERATURES BETWEEN ROOM TEMPERATURE AND 250 DEGREES C
[J].
ACTA METALLURGICA,
1966, 14 (01)
:5-+
[12]
PERSISTENT SLIP BANDS IN FATIGUED PEAK AGED AL-ZN-MG SINGLE-CRYSTALS .2. PERSISTENT SLIP BANDS IN FRONT OF STAGE-I FATIGUE CRACKS
[J].
ACTA METALLURGICA,
1982, 30 (01)
:31-35
[13]
THE CYCLIC STRESS-STRAIN BEHAVIOR OF AGE-HARDENED CU-CO AND AL-ZN-MG ALLOY SINGLE-CRYSTALS
[J].
MATERIALS SCIENCE AND ENGINEERING,
1981, 48 (01)
:91-106
[14]
WILHELM M, 1979, 5TH P INT C STRENGTH, P1089
[15]
WILHELM M, 1979, FATIGUE MECHANISMS, P214
[16]
MODEL FOR FATIGUE OF COPPER AT LOW PLASTIC STRAIN AMPLITUDES
[J].
PHILOSOPHICAL MAGAZINE,
1974, 30 (04)
:719-738