EFFECTS OF PROCESS HISTORY AND AGING ON THE PROPERTIES OF POLYIMIDE FILMS

被引:31
作者
DENTON, DD [1 ]
BUNCICK, MC [1 ]
PRANJOTO, H [1 ]
机构
[1] UNIV WISCONSIN,MAT SCI PROGRAM,MADISON,WI 53706
基金
美国国家科学基金会;
关键词
D O I
10.1557/JMR.1991.2747
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Polyimide is used extensively in a variety of integrated circuit packaging applications. It is a good dielectric material with excellent planarizing capabilities, but like most polymers, it absorbs moisture. This hygroscopic behavior can lead to reliability problems in integrated circuit packages. The effects of variations in process history on moisture uptake are examined using gravimetric measurement techniques. In particular, the effects of cure schedule and exposure to high temperature/high humidity environments (85-degrees-C/85% RH) on steady state moisture uptake are reported. Steady state moisture uptake is shown to be a decreasing function of cure temperature. Samples cured at 250-degrees-C absorb 25% more moisture by weight than do samples cured at 400-degrees-C. Moreover, the steady state moisture uptake in polyimide is greater after the samples have been "aged" in a high temperature and humidity ambient. The bulk and surface chemical composition are also monitored as a function of aging using Fourier transform infrared spectroscopy (FTIR) and electron spectroscopy for chemical analysis (ESCA), respectively. The PI surface chemistry degrades after 700 h in an 85-degrees-C/85% RH environment. The bulk chemical composition appears to be unaffected.
引用
收藏
页码:2747 / 2754
页数:8
相关论文
共 31 条
  • [1] DYNAMICS OF POLYIMIDE CURING AND DEGRADATION - AN INSITU X-RAY PHOTOEMISSION-STUDY
    ANDERSON, SG
    MEYER, HM
    ATANASOSKA, L
    WEAVER, JH
    [J]. JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 1988, 6 (01): : 38 - 43
  • [2] MULTICHIP PACKAGING DESIGN FOR VLSI-BASED SYSTEMS
    BARTLETT, CJ
    SEGELKEN, JM
    TENEKETGES, NA
    [J]. IEEE TRANSACTIONS ON COMPONENTS HYBRIDS AND MANUFACTURING TECHNOLOGY, 1987, 10 (04): : 647 - 653
  • [3] BELLAMY LJ, 1975, INFRARED SPECTRA COM, P79
  • [4] X-RAY PHOTOELECTRON-SPECTROSCOPY ANALYSIS OF HEXAFLUORODIANHYDRIDE-OXYDIANILINE POLYIMIDE - SUBSTANTIATION FOR SUBSTITUENT EFFECTS ON AROMATIC CARBON 1S BINDING-ENERGIES
    BUCHWALTER, LP
    SILVERMAN, BD
    WITT, L
    ROSSI, AR
    [J]. JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 1987, 5 (02): : 226 - 230
  • [5] Carlson T. A., 1975, PHOTOELECTRON AUGER
  • [6] MOISTURE DIFFUSION IN POLYIMIDE FILMS IN INTEGRATED-CIRCUITS
    DENTON, DD
    DAY, DR
    PRIORE, DF
    SENTURIA, SD
    ANOLICK, ES
    SCHEIDER, D
    [J]. JOURNAL OF ELECTRONIC MATERIALS, 1985, 14 (02) : 119 - 136
  • [7] DUNTON DD, 1985, APR P INT S MOIST HU, P505
  • [8] GINSBERG R, 1984, POLYIMIDES SYNTHESIS, P237
  • [9] GINSBURG R, 1983, POLYIMIDES SYNTHESIS, V1, P237
  • [10] PREPARATION AND ADHESION OF ULTRATHIN POLYIMIDE FILMS ON POLYCRYSTALLINE SILVER
    GRUNZE, M
    LAMB, RN
    [J]. CHEMICAL PHYSICS LETTERS, 1987, 133 (04) : 283 - 287